Conceptronic Reflow cooling zone | 9 February, 2006

All,

I would like to find out if it is possible to adjust the cooling rate on a Conceptronic Reflow Oven Model HVN70. We do not use Nitrogen and the Cooloing system is Genesis GCM-1.

From profiling it seems to be cooling too quickly.

Any replies appreciated.

aj...

reply »


PWH

#39595

Conceptronic Reflow cooling zone | 9 February, 2006

I'm not familiar with the HVN70 programming but our conceptronic oven reacts well to adjusting the cooling fan speed at the end of the oven. However, TAL will likely be affected substantially by changing fan speed.

reply »

aj

#39605

Conceptronic Reflow cooling zone | 10 February, 2006

is that fan speed program controlled or manually?