Hollis PT500N Wave Solder Machine

Views: 3775

#39871

Hollis PT500N Wave Solder Machine | 22 February, 2006

I noticed some of you know info about the machine mentioned in the subject, the one on sale in the following link: http://www.equipmatching.com/used_equipment/2/40/39658.php We�d be grateful if you could help us with tech data to decide purchase, or more specifically we need to know: 1- if it is of one wave or dual wave. 2- the voltage, if it is threephase

Tks in advance!

reply »

#39904

Hollis PT500N Wave Solder Machine | 23 February, 2006

If the sales type can not provide the information you require, you are buying from the wrong company.

reply »

#39905

Hollis PT500N Wave Solder Machine | 23 February, 2006

the fact is that is an auction

reply »

#39906

Hollis PT500N Wave Solder Machine | 23 February, 2006

They should still provide you with a technical contact to answer these questions.

reply »


RDR

#39907

Hollis PT500N Wave Solder Machine | 23 February, 2006

look here for some detail on this machine It doesn't tell you if it is a dual wave but all other questions are answered. Just call this place up and ask.

http://www.equipmatching.com/used_equipment/2/40/39658.php

reply »


RDR

#39908

Hollis PT500N Wave Solder Machine | 23 February, 2006

Sorry, you already have this link

reply »

#39910

Hollis PT500N Wave Solder Machine | 23 February, 2006

Be mindful that this machine is no longer support by the mfr. Electrovert/Hollis. There may be some support by third parties in the U.K. Its not a USA designed machine. It has a stainless steel pot, so it will need a titanium liner and new solder nozzle(s) and pump(s) to run Pb Free alloy safely.

reply »

Rich

#39911

Hollis PT500N Wave Solder Machine | 23 February, 2006

I would stay clear of this machine, had one and after a few years of use gave a lot of electrical problems, they are no longer supported by electrovert for electrical spares. Ours was a dual wave with HAK, 3 phase 380 volt.

reply »

#39913

Hollis PT500N Wave Solder Machine | 23 February, 2006

Thank you for your time!

reply »

#39914

Hollis PT500N Wave Solder Machine | 23 February, 2006

tks for the information! It�s helpful.

reply »

#39915

Hollis PT500N Wave Solder Machine | 23 February, 2006