Solder joint dewetting or non wetting

Electronics Forum | Wed Nov 06 10:03:59 EST 2013 | rgduval

Hi, Peter, I'm not an authority on surface finish thickness, and it's effect on reflowing, so, I can't advise on that front. If the boards are a week old, and ENIG, I would not suspect surface contamination. It's always a consideration, of course,

Solder wetting to ENIG pads

Electronics Forum | Wed May 14 12:42:16 EDT 2008 | rgduval

Dave, Realized I didn't respond to one of your questions. We pasted and reflowed one board, with no components. This board exhibited extreme dewetting on all pads. The board was LF-HASL, and the paste was Qualitek (which we've used for approximat

Express Newsletter: dewetting enig (56)


dewetting enig searches for Companies, Equipment, Machines, Suppliers & Information

Sm t t t t t t t t net
  1 2 3 4 5 6 7 8 Next
Win Source Online Electronic parts

High Resolution Fast Speed Industrial Cameras.
PCB Handling with CE

Have you found a solution to REDUCE DISPENSE REWORK? Your answer is here.
PCB Handling Machine with CE

Software for SMT placement & AOI - Free Download.
Voidless Reflow Soldering

Training online, at your facility, or at one of our worldwide training centers"
Hot selling SMT spare parts and professional SMT machine solutions

Low-cost, self-paced, online training on electronics manufacturing fundamentals