Electronics Forum | Mon Aug 04 13:13:21 EDT 2008 | patrickbruneel
The 2009M is a water based flux and requires more preheating compared to alcohol based fluxes. After checking real chunks advice you might check if you hear sizzling when the solder touches the board (indicator that the water is not eliminated by you
Electronics Forum | Fri Feb 20 02:09:23 EST 2009 | nibirta
Hi all, I have a question regarding some wave pallets having metallic traces of Titanium. The solder mask is blistering in some locations on the PCB and I am wondering if this Titaniumn may have an influence by incresing locally the temp. Also we ar
Electronics Forum | Tue Jul 29 12:51:40 EDT 2008 | grics
I am having some problems with some of my pcbs at ive solder. We are using an ersa versaflow. It has an automated spot/spray fluxer (Interflux Pacific 2009M) , 1 preheat stage, a leaded pot/nozzel, and finally a lead-free pot/nozzel. Nozzels move, b
Electronics Forum | Thu Mar 12 03:14:14 EDT 2009 | nibirta
Thank you for support. As i promised you, I am coming back with the results. The SM used was Probimer 77 with Kester 979 flux. The supplier says that there is an incompatibility and we have changed the flux with IF2009M. Same problem! They have chan