Electronics Forum | Tue Sep 20 11:59:06 EDT 2011 | SheanDalton
Check specific gravity: According to a quick web search, the specific gravity should be 0.813 ± 0.003. If you have records of the specific gravity, compare current reading to past readings. Check pressure near stone: if you have records, compare
Electronics Forum | Mon Aug 01 10:31:34 EDT 2022 | spoiltforchoice
I'm not familiar with the machine, but isn't a KE760L an old slow "single head, single gantry" two spindle machine? Any speedup from simultaneous picking would not necessarily be that much of an improvement. Setup as you described is the way I would
Electronics Forum | Wed Oct 22 06:06:54 EDT 2008 | stanyserrao
1CA64011 and 1CAFE011 UsedBy Display 1CA??011 Cause The Vision_type in part data is expressed using hexadecimal notation ("??"). If "??" equals 1E, 64, 78, 79, AC, or FE then boundary detection could not begin because the nozzle was bent.
Electronics Forum | Wed Apr 20 18:06:37 EDT 2022 | kumarb
For future readers - just needed a little bit of lube. Many thanks to Michal & the staff @ Trans-Tec (USA) for their excellent support, as always. Please see attached. For our (dated) machine, the black dial would turn only after hitting the gym
Electronics Forum | Sat May 29 16:56:26 EDT 1999 | Jeff Sanchez
| | I have always thought it to be a good practice to wash SMA's with water soluble paste (WS609) soon after reflow. Is there a time limit as to how long a board should sit after reflow before washing said board? For instance; processing a double-
Electronics Forum | Sun May 30 10:15:34 EDT 1999 | Vic Lau
| | | | I have always thought it to be a good practice to wash SMA's with water soluble paste (WS609) soon after reflow. Is there a time limit as to how long a board should sit after reflow before washing said board? For instance; processing a dou
Electronics Forum | Sun May 30 18:52:35 EDT 1999 | Graham Naisbitt
| | | | | | I have always thought it to be a good practice to wash SMA's with water soluble paste (WS609) soon after reflow. Is there a time limit as to how long a board should sit after reflow before washing said board? For instance; processing a
Electronics Forum | Mon May 31 15:09:56 EDT 1999 | JohnW
| | | | | | | | I have always thought it to be a good practice to wash SMA's with water soluble paste (WS609) soon after reflow. Is there a time limit as to how long a board should sit after reflow before washing said board? For instance; processi
Electronics Forum | Mon May 31 15:10:14 EDT 1999 | JohnW
| | | | | | | | I have always thought it to be a good practice to wash SMA's with water soluble paste (WS609) soon after reflow. Is there a time limit as to how long a board should sit after reflow before washing said board? For instance; processi
Electronics Forum | Wed Apr 28 15:51:52 EDT 2021 | duchoang
Could you share some pictures? Without any flux or paste, how could you place preforms on pads? SMT Pick and Place ?