Electronics Forum | Fri Oct 03 07:49:18 EDT 2003 | mk
Mask Musings. Soldermask (SM) and its functions have changed and evolved over the years. As an ex-solder mask applicator, I can remember screening Colonial High Gloss Epoxy soldermask on boards back in the early 80's, ending up with a thickness that
Electronics Forum | Thu May 28 07:25:58 EDT 1998 | Earl Moon
| Hey yooze guys! | Enough of the jokes between you and Earl (GRIN), let's get back to the topic...well, okay... you can tell a few more...(but good ones, 'kay?) | Anyhoo...I'm not sure if ya'll are on the IPC Technet list or not, I've not seen any p
Electronics Forum | Thu May 28 05:43:33 EDT 1998 | Earl Moon
| Hey yooze guys! | Enough of the jokes between you and Earl (GRIN), let's get back to the topic...well, okay... you can tell a few more...(but good ones, 'kay?) | Anyhoo...I'm not sure if ya'll are on the IPC Technet list or not, I've not seen any p
Electronics Forum | Tue Nov 24 05:23:18 EST 2009 | prodivegsr
Hi Davef, Thanks...Saw 1 of your thread that you posted : Thanks for providing... From davef : There are many possibilities: * Conformal coat is incompatible with surface residue on the board * Conformal coat is incompatible with solder mask on the
Electronics Forum | Wed Jun 30 10:37:11 EDT 1999 | Boca
We are wave soldering some fabs with a lot of unmasked trace area along the edges. The trace area is solid copper covered with tin / lead, no masking, no components along the edges, same on solder side and component side (goofy board design). Inste
Electronics Forum | Sat Mar 20 00:58:10 EST 1999 | Mike C
| After rmoving a BGA (plastic)to correct unexplained shorts | I installed another BGA using flux only. | Checking on an X Ray machine and found two shorts. | | can anyone give a good explenation ? | | Thanks | | Ron | Another possibility Via's n
Electronics Forum | Wed Jun 30 12:14:40 EDT 1999 | John Thorup
| | We are wave soldering some fabs with a lot of unmasked trace area along the edges. The trace area is solid copper covered with tin / lead, no masking, no components along the edges, same on solder side and component side (goofy board design). I
Electronics Forum | Wed Jun 30 11:38:05 EDT 1999 | Brian Conner
| We are wave soldering some fabs with a lot of unmasked trace area along the edges. The trace area is solid copper covered with tin / lead, no masking, no components along the edges, same on solder side and component side (goofy board design). Ins
Electronics Forum | Fri Jul 02 10:06:17 EDT 1999 | John Thorup
| | | | We are wave soldering some fabs with a lot of unmasked trace area along the edges. The trace area is solid copper covered with tin / lead, no masking, no components along the edges, same on solder side and component side (goofy board design)
Electronics Forum | Fri Jul 02 09:54:02 EDT 1999 | John Thorup
| | | | We are wave soldering some fabs with a lot of unmasked trace area along the edges. The trace area is solid copper covered with tin / lead, no masking, no components along the edges, same on solder side and component side (goofy board design)