Electronics Forum: ultrasonic bonding (Page 1 of 4)

gold wire bonding

Electronics Forum | Wed Dec 28 03:33:31 EST 2005 | sparrow

I would like to know if ENIG is widely used for the thermosonic gold wire bonding or this application is an exotic one. And I also wold like to talk to someone who uses printed circuits with ENIG finish for such an application. I do not quite underst

soldering and bonding on gold PCB's

Electronics Forum | Mon Jan 07 20:37:15 EST 2002 | davef

For soldered areas, we like to keep gold thickness substantially below the maximum you propose. Search the fine SMTnet Archives for our discussions on the topic of acceptable levels of gold with solder connections. Let�s fix this �no one seems be s

Contaminants after SMT which affect wire bonding

Electronics Forum | Fri Oct 06 04:23:06 EDT 2006 | David

What is the solder finish of the board?. If this is gold, maybe you should check the reflow profile and max temperature which can easely kill your gold coating so problems with bonding. Also we are using Prozone Multicore with ultrasonic to clean

soldering and bonding on gold PCB's

Electronics Forum | Wed Jan 09 12:20:00 EST 2002 | mregalia

Thanks for cluing me into IPC-2221. Though the numbers they give seem to contradict what I have learned from people working with the materials. At least I now know where the guideline for a max of 30 microinches of gold for soldering comes from. But

aluminium wire bonding on Electroless Nickel + Immersion gold

Electronics Forum | Mon Aug 27 15:06:29 EDT 2001 | davef

This otta push Wolfgang over the top ... Recommended reading G.G. Harman, Wire Bonding in Microelectronics : Materials, Processes, Reliability, and Yield, 2nd edition, McGraw-Hill Electronic Packaging and Interconnection Series, 1997. G.G. Harman, R

aluminium wire bonding on Electroless Nickel + Immersion gold

Electronics Forum | Fri Aug 17 01:40:55 EDT 2001 | V.RAMANAND KINI

We are in the watch & clock Business. We have a Watch IC chip that has to be wirebonded using Ultrasonic aluminium wedge bonder. The wire dia is 1.25mil. The PCB is made of G10 Glass epoxy copper clad laminate. The copper thickness is 18 microns. The

wirebonding

Electronics Forum | Thu Sep 08 07:04:02 EDT 2005 | davef

Finer pitch: Wedge bonding can be designed and manufactured to very small dimensions, down to 50 mm pitch. Processing speed: Machine rotational movements make the overall speed of the wedge bonding process less than thermosonic ball bonding. Alumin

temperature induced IMC in wire bonds?

Electronics Forum | Tue Nov 15 09:31:27 EST 2005 | arclightzero

I have been reading a good deal about IMC (purple plague in particular) in gold wire/aluminum pad wire bonds. My company uses ultrasonic wedge bonding, and for the most part all of our bonding is gold/gold, however we have one particulr part that has

Intercomnect Characterization

Electronics Forum | Wed May 31 05:32:14 EDT 2000 | F.Frimpong

Hi All, I am looking to design some test structures on GaAs and High resistivity silicon for the high frequency characterization of interconect materials. (Organic substrate, vrs LTCC, Flipchip bump configuration: (metallurgy, shape height etc) conta

How actually the process of Electrofoam Stencil?

Electronics Forum | Fri Jan 07 03:04:12 EST 2005 | Deepak Mudliar

Following are my queries : 1. How actually the process of electrofoam Stencil preparation? 2. How N2 Helps for Leadfree soldering ? 3. Does Ultrasonic Cleaning process affects the internal bonding of IC ?

  1 2 3 4 Next

ultrasonic bonding searches for Companies, Equipment, Machines, Suppliers & Information

Sell Used SMT & Test Equipment

High Precision Fluid Dispensers
Electronic Solutions

High Throughput Reflow Oven
Software for SMT

World's Best Reflow Oven Customizable for Unique Applications