Electronics Forum | Tue Aug 20 11:24:46 EDT 2002 | yngwie
Experts, Is there any reference to the best wetting time when doing manual soldering in order to get the most reliable joints i.e to avoid thick intermetallic line formations. I heard people says, the shorter the better, but how short is short...sa
Electronics Forum | Wed Aug 21 10:20:05 EDT 2002 | ksfacinelli
Dave, I am interested in a amine hydrochloride activated flux. Can you give suggestions on readily available fluxes that you have used that have strong deoxidization properties. I am looking at something that could be used in a pinch when the stan
Electronics Forum | Tue Aug 20 21:46:09 EDT 2002 | davef
Rinse => OSP Coat => Rinse => Dry Hot Air Solder Level: Preclean => Rinse => Flux Coat => Solder Coat => Hot Air Level => Cool => Soft Brush => Post Clean Rinse => Dry Look here http://www.epa.gov/opptintr/dfe/pubs/pwb/ctsasurf/download/pdf/ch2.pdf
Electronics Forum | Tue Aug 20 22:37:15 EDT 2002 | dwoon
I notice that dip fluxing method is commonly used in flip chip assembly (FCOB, FCOC and FCOF). Main reason: better flux control. How about spray fluxing (e.g. the non-contact jetting technology from Asymtek)? Does anyone has experience adopting thi
Electronics Forum | Wed Aug 21 18:11:47 EDT 2002 | dragonslayr
..and the choir is humming in 5 part harmonies. Personnally, I never gave much truck to Cpk stuff. Seems to be a high falutin way of showing the lowerlings that academics can manipulate numbers. Dazzle 'em with brilliance or baffle 'em with bull puke
Electronics Forum | Wed Aug 21 19:22:44 EDT 2002 | stownsend
Splitting hairs is putting it mildly. I�m just trying to rule out all variables. It doesn�t appear that we have an SIR problem, but since the newest variable is OSP (blame the new guy for all the problems), I have to consider it. I�ve seen this befo
Electronics Forum | Tue Aug 27 22:01:37 EDT 2002 | davef
IPC [search the fine SMTnet Archives for links] sells 7530 and other documents like it. The frequency that you check your temperature profile depends on: * Confidence that your oven is holding the profile. * Purpose of running the profile, for insta
Electronics Forum | Thu Aug 22 07:48:30 EDT 2002 | Dave Milk
While separating individual pcbs from a panel, operators have caused delamination of the edge of the board, at the tabs that were cut. How can these boards be repaired? The delamination causes them to fail J-STD-001C 9.2.1.1.d. Also, what would yo
Electronics Forum | Thu Aug 29 13:54:54 EDT 2002 | MikeF
I prefer to eat my crunchy Cheetos while drinking a cold Southpaw Light, at home. My second choice is a Mountain Dew and Cheetos in the afternoon to get me through the rest of the day. All y'all have a good holiday weekend. Mike F
Electronics Forum | Sun Aug 25 17:25:03 EDT 2002 | jersbo
Hi Chris... Funny no one has answered ,,,, read the fine SMTNET archives or Read the paste MFGs spec hehehehe.... but anywho... it really depends on the paste MFG and/or your RH conditions in house... from experience... I can say 3-5 hours.. Most p