Bubbles in Conformal Coating

Electronics Forum | Thu Jan 22 09:04:22 EST 2009 | mefloump

Humiseal recommends a 1 to 1 mix ratio of 1B31 and Thinner 521. I have for that I need to thin my ratio more to get humiseal to spray correctly in our PVA650. Also I am using Humiseal 1B73 but the tech data sheets say the same for spraying. Try thinn

Acrylic Coating De-Wetting?

Electronics Forum | Tue Jul 25 16:08:52 EDT 2017 | dontfeedphils

I'm currently working on bringing a manual coating process/workcenter online and my QA team is giving me some grief. For background, we're using Humiseal 1B31 thinned with thinner 521, mixed at 1:1 by volume. Spraying through a Binks HVLP with 10 P

Bubbles on solder joint(after conformal coating curing)

Electronics Forum | Fri Dec 18 09:07:24 EST 2009 | tommyg_fla

dave, where I work they are having the same problems with 1B31 acrylic. The coating thickness is 6-8 mils dried so that have to do several passes with an air dry between them and a final oven cure. They think that it might be related to the heating r

Conformal coating mask dots and halos

Electronics Forum | Thu Feb 25 07:37:42 EST 2010 | pcbrown

We are using Humiseal 1B31 and polyester dots for masking. We are spraying this in a Binks sprayer mixed at almost 1:1 with 521 thinner. Whe are seeing the coating creating thin halos around the poly dots as if the dots are "rejecting" the coating. T