In Section 5.1 Flux Residues, 5.2 Particulate matter 5.3 Chlorides and Carbonates & White Residues, I am assuming that these boards have been through some type of cleaning step. Hot water, saponifier, air dryed and the pictures illustrate unacceptab
Electronics Forum | Wed Oct 17 09:13:50 EDT 2012 | sfeinsp
How to turn OFF message "Solder Insp OFF" on Mirtec 4.5.5.0 program
Electronics Forum | Tue Aug 02 06:30:04 EDT 2016 | technotronix
I think it is normally from 4.0 to 5.0
Electronics Forum | Wed Jun 03 22:07:41 EDT 2009 | davef
= 0.66 aperture opening to the stencil wall has been shown to provide the best transfer efficiency and repeatability of the deposited paste. Values from 0.66 to 0.8 insure a good paste release from the stencil. The biggest impact on area ratio is the
Electronics Forum | Mon Jan 23 22:53:31 EST 2012 | davef
= 0.66 aperture opening to the stencil wall has been shown to provide the best transfer efficiency and repeatability of the deposited paste. Values from 0.66 to 0.8 insure a good paste release from the stencil. The biggest impact on area ratio is the
Electronics Forum | Wed May 19 10:35:37 EDT 1999 | Jeffrey L. Gumm
Trying to find a manufacturer with the capability to hold a registration tolerance of +/- .001" in LPISM. To be done on ceramic substrates, with a maximum panel size of 5.0" x 7.0".
Electronics Forum | Sat Jan 29 23:55:58 EST 2005 | KEN
I recently ran a process evaluation (Print/ P&P /Reflow) and was plesently surprised with a 5.0 sigma process or 250ppm. Attrition was under 1%. Keep in mind this is defects counted Post-reflow. The most signifficant defect was tombstoning / draw-
Electronics Forum | Wed Jan 17 18:42:49 EST 2007 | Richard
I'm trying to get an even solder coating onto a retangular shaped ceramic substrate (5.0mm x1.83mm), but the solder tends to pool on the short side of the substrate.