Electronics Forum | Thu Sep 26 13:35:28 EDT 2002 | jersbo
Thanks to everyone who posted! I did get the boards clean and it worked well I used AIMTERGE 520A about 5% in HOT water.. I soaked for 10 minutes used a brush(handscrubber type)to loosen the residue. For the fine pitch I used a fine bristled small
Electronics Forum | Mon May 26 11:02:17 EDT 2008 | jandon
Hi Mr. Necdet Ozyonum, Recently we did have same kind of problems when we use lead free reflow profile for leaded solder paste (AIM WS-483). There where solder resist lacks, we found white residue after aqueous cleaning. Not in the solder joints but
Electronics Forum | Tue Sep 03 17:48:34 EDT 2002 | dphilbrick
My customer is finding a blue haze on some SMT pads after processing, kind of looks like a water spot on the surface of solder joints. It requires 20x mag and very good lighting to see. We have done 2 different ionic tests and the boards pass to clas