Electronics Forum | Thu Aug 27 02:55:11 EDT 2009 | smtirl
Alloy is Sn/Pb on a HASL finish. Standard no-clean flux reflowed in Nitrogen.
Electronics Forum | Wed Sep 16 09:25:26 EDT 2009 | clampron
Are you using a SAC305 or high tin alloy? That will corrode the solder tip as well. Chris
Electronics Forum | Wed Sep 16 09:58:23 EDT 2009 | geb
Its SAC305 paste. Will that corrode the tip or the tin alloy?
Electronics Forum | Tue Apr 19 15:01:03 EDT 2011 | rdoss
Not sure who you've already looked at, but i know Alpha Metals has preforms.
Electronics Forum | Thu Apr 21 15:04:00 EDT 2011 | smt_guy
Indium Corpo of America is selling preforms..
Electronics Forum | Fri Apr 22 10:51:49 EDT 2011 | blnorman
Kester sells preforms.
Electronics Forum | Fri Apr 29 09:42:27 EDT 2011 | andrzej
Thank you all for feedback
Electronics Forum | Sat Nov 26 04:48:55 EST 2011 | rajeshwara
Better you alos take look at Cookson Alpha SACX0807 / SACX0107 alloy
Electronics Forum | Sat Nov 26 04:49:00 EST 2011 | rajeshwara
Better you alos take look at Cookson Alpha SACX0807 / SACX0107 alloy
Electronics Forum | Fri Jan 18 12:25:46 EST 2013 | tombstonesmt
The risk is that your chemistry will be off.. Don't do it..