Pb Free Voids

Electronics Forum | Wed Feb 14 02:38:13 EST 2007 | Wayne

The middle of the BGA has to make sure it has 235 deg C (if you are using SAC paste), otherwise it will not form good joint.

non-wetting

Electronics Forum | Fri May 17 22:25:51 EDT 2002 | xzinxzin

*the other components are 0402 and SOIC 16, the solderability were good. *the protection on the terminations of microleadframe package is Cu(copper),somebody call that leadless leadframe package(LLP). *the time above 210 deg C is about 10 sec. *I us

non-wetting

Electronics Forum | Tue May 21 06:33:37 EDT 2002 | hayashi

*the other components are 0402 and SOIC 16, the > solderability were good. *the protection on the > terminations of microleadframe package is > Cu(copper),somebody call that leadless leadframe > package(LLP). *the time above 210 deg C is about

Humidity of SMT component storage environment.

Electronics Forum | Tue Jan 23 09:03:00 EST 2001 | fmonette

This guideline is actually in the IPC/JEDEC standard J-STD-033, May 1999 (although it is not spelled out very clearly, thus the current confusion in the industry). The technical reason is that moisture diffusion is a very slow process. Once parts ha

  1  

c.if searches for Companies, Equipment, Machines, Suppliers & Information

Voidless Reflow Soldering

Benchtop Fluid Dispenser
Fluid Dispense Pump Integration

Reflow Soldering 101 Training Course
Pillarhouse USA for handload Selective Soldering Needs

World's Best Reflow Oven Customizable for Unique Applications
SMT feeders

MSD Dry Cabinets


MIRTEC - the Global Leader in PCB INSPECTION Technology.