Electronics Forum | Wed Jun 03 07:13:27 EDT 1998 | Tom Tellinghuisen
| We have experienced poor adhesion of acrylic conformal coating to plastic bodied IC�s. The observed symptoms of this are a blistering or lifting of the coating at the surface of the component, although peel testing has revealed that this is not al
Electronics Forum | Tue Jun 02 17:36:43 EDT 1998 | Chris Fontaine
| | We have experienced poor adhesion of acrylic conformal coating to plastic bodied IC�s. The observed symptoms of this are a blistering or lifting of the coating at the surface of the component, although peel testing has revealed that this is not
Electronics Forum | Wed May 27 21:05:30 EDT 1998 | Steve Gregory
Hey yooze guys! Enough of the jokes between you and Earl (GRIN), let's get back to the topic...well, okay... you can tell a few more...(but good ones, 'kay?) Anyhoo...I'm not sure if ya'll are on the IPC Technet list or not, I've not seen any posts f
Electronics Forum | Mon Sep 17 17:09:32 EDT 2001 | jschake
Flux: No-clean pastes tend to have a wider print process window in terms of print speed and pressure. More importantly, no-clean pastes are more tolerant to changes in temperature and humidity. They also exhibit longer stencil life than water-solub
Electronics Forum | Tue Mar 26 21:02:48 EST 2002 | Mike Konrad
There are two basic technologies to choose from: 1. Ultrasonic 2. Spray-in-air Makers of ultrasonic stencils include: Aqueous Technologies (that�s us): http://www.aqueoustech.com PMR: http://www.pmrsystems.com JNJ Industries: http://www.jnj-
Electronics Forum | Thu Aug 01 13:04:57 EDT 2002 | gdstanton
Its interesting. It appears I'm getting conflicting feeback from Indium. This says its not a problem... http://indium.custhelp.com/cgi-bin/indium.cfg/php/enduser/std_adp.php?p_sid=kTDKGClg&p_lva=&p_faqid=355&p_created=1014734692&p_sp=cF9ncmlkc29
Electronics Forum | Tue Aug 20 18:15:02 EDT 2002 | davef
Haaaaa!!!! Soldering to plastic!!!! An apt analogy!!! I like to compare it to soldering to dirt. Some thing. In fact, you are soldering on nickel, when soldering on many things. It�s just that the gold, er Pd, flash enables the wetting mechanism
Electronics Forum | Thu Nov 13 17:18:11 EST 2003 | davef
First, don�t get distracted by �OA� and �NC� formulations. This is nomenclature. We want to discuss the issue of �activity�. J-STD-004 "Requirements for Soldering Fluxes" classifies fluxes by their chemical composition, activity level and halide c
Electronics Forum | Sat Jun 12 00:34:00 EDT 2004 | kanwal324
Hi ! The main problem being faced currently is formation of solder balls - to be precise, these are micro solder beads generally found attached with bodies of SOTs, Chip Caps, Chip Resistors, between pins of SOICs (50 mil) - lying on PCB surface,
Electronics Forum | Fri Mar 18 15:02:07 EST 2005 | pmd