Electronics Forum | Mon Sep 28 12:25:13 EDT 2009 | vleasher
Could someone point me in the direction of some good manufactures of batch style curing ovens? We have a new project requiring Humiseal 2A64 and we do not have an oven for the 3hrs @ 170F cure. Thanks in advance!
Electronics Forum | Mon Sep 28 15:36:29 EDT 2009 | davef
While you're waiting for others to reply, search the fine SMTnet Archives to find threads like: http://www.smtnet.com/Forums/Index.cfm?CFApp=1&Message_ID=56260
Electronics Forum | Tue Apr 13 23:27:34 EDT 1999 | Mike Flori
I need to cure conformal coat on a 19" x 15" board. The material needs 7 - 10 minutes at 100deg C, but I have limited floorspace so I'm looking for an oven with about 36 inches heated length and 18 or more inch wide belt. The material we are consider
Electronics Forum | Wed Apr 14 17:13:08 EDT 1999 | Stephen Oltmann
| I need to cure conformal coat on a 19" x 15" board. The material needs 7 - 10 minutes at 100deg C, but I have limited floorspace so I'm looking for an oven with about 36 inches heated length and 18 or more inch wide belt. The material we are consid
Electronics Forum | Wed Apr 14 17:14:49 EDT 1999 | Stephen Oltmann
Check with BTU. They have dryers in the length you need. Good luck! | | I need to cure conformal coat on a 19" x 15" board. The material needs 7 - 10 minutes at 100deg C, but I have limited floorspace so I'm looking for an oven with about 36 inches
Electronics Forum | Sat Apr 17 11:56:04 EDT 1999 | Graham Naisbitt
Mike First, you MUST make sure the oven used is extracted. The coating will contain TDI. This is not nice. You would be better considering a silicone solventless. Try contacting HumiSeal. They had a material on the TAC line at Nepcon West that lo
Electronics Forum | Wed Apr 14 20:39:02 EDT 1999 | Dave F
| I need to cure conformal coat on a 19" x 15" board. The material needs 7 - 10 minutes at 100deg C, but I have limited floorspace so I'm looking for an oven with about 36 inches heated length and 18 or more inch wide belt. The material we are consid
Electronics Forum | Fri Apr 17 14:08:00 EDT 2015 | davef
Humiseal says, "UV cure – These materials are also more difficult to repair as they are the most chemically resistant and mechanically tough of all conformal coatings. Removal is possible locally by using powder abrasion."
Electronics Forum | Fri Apr 17 08:52:03 EDT 2015 | charliedci
Thanks for the info Sarason. The UVCL is a Urethane. Did not want that hard of finish (for solder rework issues). We like the Acrylic as acetone will remove cured material for solder rework.
Electronics Forum | Thu Mar 31 10:14:06 EST 2005 | davef
There's some nice low-VOC uV coatings out there. We don�t use uV cured coatings, but try: * http://www.emersoncuming.com * http://www.dymax.com * http://www.mgchemicals.com * http://www.loctite.com * http://www.humiseal.com Be aware that uV co