detection of cold solder

Electronics Forum | Tue Sep 14 06:00:27 EDT 2004 | sc

dear, appreciate the sharing of experience on detection tools of cold soldering defect on PCBA. thanks SC

detection of cold solder

Electronics Forum | Tue Sep 14 06:00:31 EDT 2004 | sc

dear, appreciate the sharing of experience on detection tools of cold soldering defect on PCBA. thanks SC

detection of cold solder

Electronics Forum | Wed Sep 15 11:44:46 EDT 2004 | mriddle

Dear SC, Are you looking for a cold solder detection tool for SMT,through-hole or both?

cold joint on 1 lead of IC

Electronics Forum | Mon Feb 12 10:02:18 EST 2007 | rgduval

A little late to the party here, sorry... Has the joint been verified as a cold solder joint? That is, visually confirmed that it looks like cold solder, and, perhaps, xrayed to confirm the solder status? X-raying may sound a bit extreme, but you'

BGA Rework affected by cold weather?

Electronics Forum | Thu Dec 04 10:59:02 EST 2014 | rrosera

HI, I work for a company in New England and recently had a unusually large number of boards fail after replacing a BGA on them. We use a AirVac DRS25 to remove and replace the BGA witch uses local forced hot air. We usually have at least a 90% s

cold solder after drop test

Electronics Forum | Wed Jan 07 07:16:25 EST 2004 | davef

Cold solder prior to properly performing a well designed drop test. Actually, "cold solder" means different things to different people. Two dull solder connection conditions are: * "Disturbed" solder joint: a solder joint that has an "angular face

cold solder after drop test

Electronics Forum | Tue Jan 06 19:53:32 EST 2004 | jj

Hi, Any idea what's the possible causes of cold solder after drop test? Thanks JJ

cold solder at flexible pcb

Electronics Forum | Thu Aug 12 21:06:48 EDT 2010 | ptpaazmi

COLD SOLDER LOCATION U600/U601 Problem : Several XMp3i Rotary swithes were found to exibit intermittent function during a DV build at WNC

cold solder at flexible pcb

Electronics Forum | Tue Aug 24 20:15:27 EDT 2010 | davef

What is ... and how does it pertain? * Location U600/U601 * XMp3i Rotary swithes * DV build * WNC

facing cold joint problem

Electronics Forum | Sun Jan 18 10:13:59 EST 2004 | davef

Materials added to solder can change its appearance. For instance: * Gold in tin/lead solder is dull / grainy * Palladium in tin/lead solder is dull / grainy We do NOT advocate using visual appearance to define the appearance of a good and a bad so

  1 2 3 4 5 6 7 8 9 10 Next

cold solder inspection searches for Companies, Equipment, Machines, Suppliers & Information

INSPECTION TECH
INSPECTION TECH

Our Company handle AOI (Auto Optical Inspection) and SPI (Solder Paste Inspection) Machines.

Equipment Dealer / Broker / Auctions

Hwaseong-si, Gyeonggi-do, Korea
Hwaseong-si, South Korea

Phone: +82-1029254936

Voidless Reflow Soldering

High Resolution Fast Speed Industrial Cameras.
Pillarhouse USA for Selective Soldering Needs

High Precision Fluid Dispensers
Pillarhouse USA for handload Selective Soldering Needs

High Throughput Reflow Oven
Best SMT Reflow Oven

World's Best Reflow Oven Customizable for Unique Applications


"回流焊炉"