Electronics Forum | Thu Aug 21 16:33:49 EDT 2008 | decaire
The 2 most common approaches for MSD Tracking and Control on the factory floor are: 1) Manual paper-based procedures (Example: Log Sheet or Label that the operator must fill out and pay attention to) - or - 2) Software-based tracking system (Example
Electronics Forum | Fri Oct 03 07:49:19 EDT 2008 | grantp
Hi, I just saw the new NXT machines at globaltronics in Singapore, and mostly they are faster. However what was interesting is Fuji shows a prototype of the new XPF machine, but it was called XPF-W which handles really large PCB's and uses the sam
Electronics Forum | Thu Feb 12 15:32:15 EST 2009 | gtemkin
A few other data points to consider. My experience working with Dymax 984LVF material was that its UV cure must be initiated immediately after coating, otherwise is surface will remain tacky forever, something like a post-it note tackiness, which wi
Electronics Forum | Thu Jul 09 08:34:14 EDT 2009 | rway
Hi, do you know where and how we can tests 0402 > ceramic capacitors? We would like to test them > individually before we place them on our board; > so as to get some test yield and the distribution > of the parameters of this component based on
Electronics Forum | Tue Aug 18 22:22:43 EDT 2009 | comatose
Assuming you want to run 8 hours a day and 5 days a week, you need a sustained throughput of 2.5k components per hour. With fine pitch, futzing around, setup, etc you should really look for machines rated in the 4k to 5k per hour range. That's not sc
Electronics Forum | Tue Aug 18 10:11:04 EDT 2009 | grantp
Hi, Yes, I think this sounds like a form of tomb-stoning, and we used vapor phase until it ended up driving us totally nuts trying to deal with tomb-stoning. We tried everything, and all kinds of stencil apertures. Vapor phase is an amazing process
Electronics Forum | Thu Nov 19 05:18:37 EST 2009 | prodivegsr
Hi All, Recently we are working on the conformal coating process using Humiseal chemical 1B73 and thinner 521. Bubbles on component body/joints are seen after gone through the IR Reflow Oven. During the conformal coating, only tiny bubbles seen af
Electronics Forum | Fri Mar 26 15:36:50 EDT 2010 | krish_bala
Hello Graham, We are currently using Tacky Gel Flux during our replacement process. We dip the BGA component on the flux prior to placement. Once it is dipped, the alignment and placement is done. As for the profile, I believe I am hitting the corr
Electronics Forum | Wed Jun 22 18:52:56 EDT 2011 | semiconjt
tTo explain what I mean...sorry for my bad Engilsh... please find short " patchwork stencil" description from EPP Europe. http://www.epp-online.de/europe/-/article/16537487/15944614/Innovators-of-laser-processing-technology /art_co_INSTANCE_0000/max
Electronics Forum | Sat Oct 22 22:10:09 EDT 2011 | unisoft
Hi maybe this will help Rich larue rlarue@unisoft-cim.com ProntoGERBER-CONNECTION ( http://www.unisoft-cim.com/gerber_connection.htm ) imports raw Gerber data and allows the user to add intelligent information to the shapes on the display and c