Electronics Forum | Wed Mar 28 01:13:11 EST 2001 | Mike Konrad
Hi Kerry, I also am glad that we have the opportunity to discuss the EPA �certification� with regards to equipment and chemistries. I also have contacted the EPA with specific questions concerning the program you are promoting. The EPA responded t
Electronics Forum | Thu Mar 29 13:06:07 EST 2001 | billschreiber
Hello again Mike, First, I apologize to the people that have been put through this exercise. However, I cannot let you continue to misrepresent my company. Your continued attempt to cloud this issue by referring solely to the U.S. EPA�s Verificati
Electronics Forum | Wed Apr 11 14:05:30 EDT 2001 | davef
No, there's not a really great epoxy product for attaching thermocouples in reflow. Specifically, what's your problem? From Sanders Temprobe verbage ... Adhesives There are two general classes of material commonly used to adhesive bond thermoc
Electronics Forum | Sat May 12 00:04:36 EDT 2001 | zam_bri
The product I'm running currently consist a mix of 20 mil pitch QFP, 50 mil pitch, 0402, BGA and variable size of connectors from small to big, on OSP finished PCB. Running intrusive reflow with a mix packages is a real headache, esplly when you hav
Electronics Forum | Fri Jun 15 14:05:20 EDT 2001 | CPI
In response No that�s not all you need to think about, but lets look at each and then talk of others. a)The condition of the solderable surface on boards (and components) degrades over time or can be supplied in poor condition (to thin or thick HASL
Electronics Forum | Thu Jul 05 19:39:19 EDT 2001 | davef
I had forgotten that it was you that was on the Sipad adventure. [But then again, who can keep track of yer aliases? ;-)] You just go from one adventure to the next. Expanding On Dave�s Hi-Test Flux Method Theory � PASTE: Yes, contact your favorit
Electronics Forum | Tue Dec 28 15:12:03 EST 1999 | Bill Schreiber
Rick, Ultrasonics is a mechanical scrubbing action (cavitation) similar to any other scrubbing action, if you scrub long enough, you stand the chance of wearing away some of the surface material (shiny coating of a solder joint). The shiny coat on a
Electronics Forum | Mon Dec 20 13:39:08 EST 1999 | Wolfgang Busko
Hi Clarissa, seems to be a real start up situation you are in. For the printing there is IMO no need to buy any sophisticated automatic-vision-alignment-self-cleaning-inline-and-more-machine. Features you need: - adjustable in X-,Y-,Z-axis (individu
Electronics Forum | Thu Nov 04 23:45:16 EST 1999 | Jeff Sanchez
Hey Brian, We are not sure what it is you are referring too? If you feel they did not respond promptly than I am assuming that you picked up the phone and asked them what's up? Your thread just came across as bashing and a little negative, as
Electronics Forum | Tue Oct 12 16:26:01 EDT 1999 | Jeff Sanchez
| | | | We have three buckets filled with leftover solder paste from our screen printing process. Kester has informed me that they no longer take paste, but only dross and pot dumpings. Does anyone know if there's someplace I can recycle this, or a