Electronics Forum | Sun Sep 12 06:49:39 EDT 1999 | Eyal Dickerman
| Hi All, | | Does any one out there have SPC control on Chip placement Machines? I was wondering what type of parameters we can monitor. We have Siplace here equip with SEC-GEM and a monitoring software. Just curious if anyone has done SPC on Chip
Electronics Forum | Thu Sep 09 15:28:20 EDT 1999 | C.K.
Hello SMTNEtters': Does anyone know of any suppliers who can supply De-I H20 (some high-quality H20!!) in 55 gallon containers. We have no use for "point-of-use" treatment, like mixed bed, anion, or cation tanks, or anything like that...we're a NO
Electronics Forum | Fri Sep 10 08:39:01 EDT 1999 | ScottM
| Hello SMTNEtters': | | Does anyone know of any suppliers who can supply De-I H20 (some high-quality H20!!) in 55 gallon containers. | | We have no use for "point-of-use" treatment, like mixed bed, anion, or cation tanks, or anything like that...
Electronics Forum | Fri Sep 03 08:12:41 EDT 1999 | Mike DEmos
I am looking for some PM software to use throughout my Electronics factory. Currently, we have a manual system consisting of check-off sheets, log-books, etc. Ideally I would like a system that would throw-up a flag (perhaps by e-mail) when PM is d
Electronics Forum | Wed Aug 25 21:51:13 EDT 1999 | Jason Tomlinson
| Does anyone have any information on stencil aperture/pad ratios for noclean solder paste. In the past I have experienced severe solder ball problems when using the same size apertures from aqueous products as I do with the No-clean products. Cons
Electronics Forum | Fri Aug 20 16:00:20 EDT 1999 | Earl Moon
| Has anybody run across a good concise book or other source on solder paste, its characteristics, handling, storage, stencil design, printing and reflow? Yes I asking for the world! | | TX | Mark | As the world turns, or is/was that a soap my x/fu
Electronics Forum | Wed Aug 18 22:01:35 EDT 1999 | Stu Leech
We have developed a new process for removing moisture from surface mount devices. We have one site where PCB laminate drying has been reduced to 1.5 hours. A standard oven took 4 hours to do the job. I am looking for a firm who does large scale board
Electronics Forum | Wed Aug 18 22:02:24 EDT 1999 | Stu Leech
| We have developed a new process for removing moisture from surface mount devices. We have one site where PCB laminate drying has been reduced to 1.5 hours. A standard oven took 4 hours to do the job. I am looking for a firm who does large scale boa
Electronics Forum | Thu Aug 19 05:42:01 EDT 1999 | Brian
| We have developed a new process for removing moisture from surface mount devices. We have one site where PCB laminate drying has been reduced to 1.5 hours. A standard oven took 4 hours to do the job. I am looking for a firm who does large scale boa
Electronics Forum | Wed Aug 18 15:56:20 EDT 1999 | david dougherty
Hadco offers a technology of building in a "buried" capacitance layer (& other embedded passives) in organic PWBs (FR4 for example). see http://www.hadco.com/prod03.htm and a design manual is posted here: http://www.hadco.com/pdfs/bcguide.pdf I am c