Electronics Forum | Mon Jun 27 20:32:46 EDT 2022 | kumarb
Absolutely..there are many suppliers of this common widget. Here are some names - we use (have met each in HK / Taipei): The 800-lb gorilla / leader of this industry: http://www.kangyang.com.tw But we found Judy (Yazhoulong) to offer the best p
Electronics Forum | Wed Sep 21 13:17:26 EDT 2022 | unisoft
Yes, the import data type is a common issue with electronics contract manufacturers and some OEM's. Unisoft ( http://www.unisoft-cim.com ) has been doing this for over 35 years. The software focuses on contract manufacturers issues and the software
Electronics Forum | Thu Oct 20 17:03:56 EDT 2022 | rgduval
As much as I love MyData machines, if you are low mix high volume, they may not be the best solution. They have their place in the mix, but, I believe their greatest value is in high mix environments. Not to say that the My's won't do the work, the
Electronics Forum | Thu Jan 12 16:53:59 EST 2023 | SMTA-67037450
I need to benchmark or sanity check our incoming inspection process in relation to IPC Class 3 electronics. I am looking for a contact with someone who assembles/builds IPC Class PCBAs, that i can sanity check some stuff with. To start, our process
Electronics Forum | Fri Mar 24 15:35:58 EDT 2023 | cyber_wolf
All of these components were replaced under warranty. I cant remember how long that was. I was working with the very first My12's. This machine was never reliable and there was always something broken. Anywhere I have ever been that had MY series mac
Electronics Forum | Fri Jul 21 12:55:32 EDT 2023 | davef
From ESD Systems [ https://esdsystems.descoindustries.com/QuestionsandAnswers/ShowQuestion.aspx?i=405 ] Antistatic Property of some Kapton® Tapes - Tribocharging when removed from a surface or unwound from the core: - 3M's Tape # 42 generates from
Electronics Forum | Mon Mar 25 21:45:22 EDT 2024 | buckeye
I got an inquiry from one of our electronics labs with regards to their soldering processes. They use eutectic (63% Sn, 37% Pb) solder. For liquid flux they are currently using Kester 186, which is an old-school, full rosin (RMA and ROL1) flux that c
Electronics Forum | Tue Mar 14 05:02:35 EST 2000 | emmanuel
I am to implement PBGA, and i am looking for PCB surface finish informations. A lot of technical reports are specifing NiAu finishing because of flatness property. Because of leads shape, I though that BGA doesn't need flat pads like QFP. Is it false
Electronics Forum | Mon Mar 13 15:10:52 EST 2000 | Stuart Adams
Assuming agressive design rules what is the minimum distance I can get away with between the board edge and a SMT pad and between the board edge and a plated mounting hole ??? (The board is only 1"x2" and the mounting holes are 80 mil dia, 125 mil
Electronics Forum | Mon Mar 13 15:35:32 EST 2000 | Ioan
Stu, it is good you know that there are limitations and you want everything. Wish our designers work like that. So, the limitations we impose are dictated by the rails of the insertion and dispensing machines. Normally a .150" keepout will make a s
Manufacturer of PCB depaneling and PCB soldering machines since 2005, products include CE approval V-groove PCB depanelizer, PCB router, PCB punching machine, laser depaneling, hot bar soldering machines and soldering robots.
Liwu Industrial Park, Yuanzhou Town, Boluo
Huizhou, China
Phone: +86-138-29839112