Electronics Forum | Tue Sep 19 09:34:33 EDT 2000 | Erick Russell
There are two places where Laser Soldering is used for rework. One is the low volume, high mix environment where the board value is high. The other is the high volume (regardless of mix) facility where fast process time and quick set-up is required.
Electronics Forum | Mon Sep 18 12:04:43 EDT 2000 | Erick Russell
Photonic Soldering is useful for several applications in rework where current methods using hot air are inadequate or inefficient. For high-density assemblies, component clearances are limited. In the past, DFM (Design for Manufacturing) specificati
Electronics Forum | Fri Sep 15 05:48:24 EDT 2000 | carsonho
Have any experience that Sn/Pb plated integrated circuit products will appear some rainbowbridge-like substance after exposing at conditions of 121degC, 100%RH and 15psi for 48hours or above? The rainbow bridge substance was analyzed by EDAX and fou
Electronics Forum | Fri Sep 15 05:48:11 EDT 2000 | carsonho
Have any experience that Sn/Pb plated integrated circuit products will appear some rainbowbridge-like substance after exposing at conditions of 121degC, 100%RH and 15psi for 48hours or above? The rainbow bridge substance was analyzed by EDAX and fou
Electronics Forum | Thu Aug 24 16:59:11 EDT 2000 | Dr. Ning-Cheng Lee
For reflowed solder joints, Bi bearing solder has been reported to exhibit superior fatigue resistance. It also provides better wetting than many other alternatives, including SnAgCu systems. In my opinion, it may be the choice once all Pb can be pha
Electronics Forum | Thu Aug 24 17:08:58 EDT 2000 | Dr. Ning-Cheng Lee
Depending on the stress condition experienced by the solder joints. For joints under a greater stress, the time to reach equilibrium can be shorter. Of course, the change is also more significant in phase structure. For low stress conditions, it may
Electronics Forum | Wed Aug 23 17:06:40 EDT 2000 | Dr. Ning-Cheng Lee
For 20 mil pitch pads, the volume control is more critical in terms of bridging concern. In general, solder paste for dispensing is more prone to slumping due to low metal load and low viscosity. If the volume dispensed is on the high end, or if the
Electronics Forum | Wed Aug 23 16:46:52 EDT 2000 | Dr. Ning-Cheng Lee
Comparing 62Sn/36Pb/2Ag with 63Sn/37Pb, addition of 2% Ag introduces two major advantages. The first advantage is grain refining, and the resultant better fatigue resistance. The second advantage is a wider processing window on Ag metallization. Pres
Electronics Forum | Wed Aug 23 16:29:16 EDT 2000 | Dr. Ning-Cheng Lee
The surface tension of solder you mentioned should be referred to as interfacial tension between solder and flux. According to Antonow�s rule, the interfacial tension is the difference in surface tension of molten solder and liquid flux. Since flux a
Electronics Forum | Wed Aug 23 16:18:47 EDT 2000 | Dr. Ning-Cheng Lee
I presume you are referring to vibration test with fixed frequency at room temperature. One procedure describing the detailed profile is in MIL-STD-883E, Method 2005.2 (12/31/96). The approximate profile can be described as 60Hz, 20-70g, and 96 hrs t
Manufacturer of PCB depaneling and PCB soldering machines since 2005, products include CE approval V-groove PCB depanelizer, PCB router, PCB punching machine, laser depaneling, hot bar soldering machines and soldering robots.