Electronics Forum | Tue Nov 26 08:51:52 EST 2019 | marwan
we're using the Balverzinn Cobar 390-RX-HT and it wery good for wave and selective soldering and he can support a verry high temperatures
Electronics Forum | Fri Nov 29 09:45:39 EST 2019 | surfacemountprocess
Have used Interflux 2005C in a Ersaflow 3-45 and happy with the results
Electronics Forum | Wed Dec 04 02:46:15 EST 2019 | collum
We use the flux Cobar 94-SEL with excellent results. It is a special flux for selective soldering process. When the temperature of the board with flux (preheating or during soldering) reach more 130°C, the rests of flux are deactivated (no more dange
Electronics Forum | Thu Nov 21 19:55:38 EST 2019 | myke03o
Would like to know what type of soldering iron you are using. On this type of big jumpers, a continuous heating soldering Iron will do the job nicely in order to heat the jumper wire properly.
Electronics Forum | Wed Nov 27 08:08:08 EST 2019 | dontfeedphils
Just make more specific shapes/packages for these size parts and decide on a naming convention that's easy to decipher then stick with it.
Electronics Forum | Thu Nov 14 22:04:09 EST 2019 | liangshimoli
dear all, sorry for interupt, but i need a big amount of UIC feeder, who have source please contact me or introduce me. my email: luong.nhai6@gmail.com Hope to see your voice. thank you!
Electronics Forum | Mon Nov 18 08:38:46 EST 2019 | davef
Go to the SMTnet "Used SMT Equipment" page [ https://smtnet.com/mart/index.cfm?fuseaction=rfq ] and submit an RFQ
Electronics Forum | Wed Nov 20 21:30:36 EST 2019 | sssamw
first of all, you need check the strain caused by interference during connector insertion. If must done by SMT, then a claw would be better than nozzle.
Electronics Forum | Wed Nov 20 01:38:53 EST 2019 | ajspec
Hi, i'm facing solder mask peel off but limited to the solder defined pad only(opening area). no peel off on the other area and it happened on electroless nickel immersion gold finishing only. for other finishing is not affected. kindly advise if you
Electronics Forum | Wed Dec 11 11:26:25 EST 2019 | SMTA-Norah
Yes, a polite complaint to our board shop later and the next batch didn't have that problem at least. I'm not convinced it's an ENIG issue as there was variability panel to panel in the first place.