Printing problem, water soluble paste with gold plating PCB..

Electronics Forum | Tue Jul 31 00:48:55 EDT 2001 | Frank

Sorry I forgot to provide enough information. Stencil thickness is 6 mil Aperture width is 10 mil Aspect ratio (aperture area / wall area) = 0.72 Solder paste mesh size, type 3 (-325 +500) With this aspect ratio we can printing without any probl

White residue VS No clean

Electronics Forum | Sun Jul 29 09:17:20 EDT 2001 | davef

Tough to say, but ... Chlorine: Many fluxes contain chlorine. Sulphur: Many solders and paper packing materials contain sulphur. Sodium: No idea. IPC-J-001 talks to board cleanliness and specifies criteria according to the cleanliness test met

Contamination test

Electronics Forum | Sun Jul 29 21:33:30 EDT 2001 | CAL

Your Ionograph and Zero-ion Values are set by you. There is no raw pass of fail criteria only the limits you set up. Ionograph is great for bare board resistivity (salt) test just as a pass fail for incoming inspection but this is all per your facto

Component soldering strength ?

Electronics Forum | Mon Jul 30 09:31:46 EDT 2001 | kennyhktan

Dear All, I'm now facing with 0805's component missing problem at the production after mounting. In able to containing the defect I'm been trying to increase the soldering strength by changing the stencil thickness from 6mil to 8 mil on a step do

Tooling Support

Electronics Forum | Tue Jul 31 03:06:11 EDT 2001 | Lex WW

I am planning to evaluate DEK's Formflex board support system in our plant soon. Does anyone have experiences with this? I know that the grid of pins "locks on" to a particular product after the initial setup, but am curious to know how each individu

Tooling Support

Electronics Forum | Fri Aug 03 12:24:14 EDT 2001 | hinerman

I can only describe how the Grid Lok handles component variability. The compliant caps have an annular ring that is very soft and can mold to different shapes. If a component shows up where there was no component before, the outside of the cap bend

Tooling Support

Electronics Forum | Thu Sep 20 13:28:23 EDT 2001 | ohanlon

Here is how the FormFlex system conforms to component variations. The FormFlex system utilizes an oil chamber that is common to ALL the pins once the system is set. Pushing down one pin will cause the displaced oil to be shared by all the others pins

Support Fixtures or Systems

Electronics Forum | Mon Jul 30 10:44:37 EDT 2001 | hinerman

A few of the more common defects If bridging or insuffienct deposits occur on the printer, one of the first things to check is the tooling. Misplaced hard tooling pins or poorly designed fixtures have a nasty habit of breaking components on side

What is the std Resistivity for DI water at Aqueous

Electronics Forum | Tue Jul 31 13:55:27 EDT 2001 | mparker

Maintain DI water to 18 Meg Ohms resistivity. You can go down as low as 2 Meg ohms, in a pinch, but I would caution on what type of board you are running if trying to clean on 2 Meg ohm. Anything that is running an RF or high frequency circuit could

What is the std Resistivity for DI water at Aqueous

Electronics Forum | Tue Jul 31 20:05:11 EDT 2001 | davef

There is no the industry standard specification for resisitivity monitoring at aqueous cleaning. Beyond those posted here earlier by Mikie, guidelines can be found in the fine SMTnet Archives, for instance: (http://www.smtnet.com/Forums/Index.cfm?CF


electronics searches for Companies, Equipment, Machines, Suppliers & Information

Nordson Electronics Solutions
Nordson Electronics Solutions

Nordson Electronics Solutions makes reliable electronics an everyday reality. Our ASYMTEK, MARCH, and SELECT brands deliver precision fluid dispensing, conformal coating, plasma treatment and selective soldering equipment.

Manufacturer

2747 Loker Ave West
Carlsbad, USA

Phone: 18002796835