Electronics Forum: enig and reflow and profile (Page 1 of 13)

Intermetallics and reflow profile

Electronics Forum | Tue May 02 15:29:14 EDT 2000 | M. F. Roe

I am looking for public papers or articles on intermetallic formation as a function of reflow profile. Most solder paste vendors specify peak temperature and time above liquidus, but I am particularly interested in what happens to intermetallic grow

Re: Intermetallics and reflow profile

Electronics Forum | Wed May 03 20:24:22 EDT 2000 | Dave F

MF: I know of nothing that addresses your question directly. Let me suggest: * Technical types at your solder supplier should be able to help. * "Effect Of Intermetallic Compounds On The Thermal Fatigue Of Surface Mount Solder Joints" PL Tu, et a

01005 components and reflow profiles

Electronics Forum | Mon Apr 16 10:01:03 EDT 2012 | patrickbruneel

*Like*

01005 components and reflow profiles

Electronics Forum | Mon Apr 16 20:04:24 EDT 2012 | hegemon

6 or 7 replies and 3 *flamer* ratings already? And here I thought this was good info above...

01005 components and reflow profiles

Electronics Forum | Mon Apr 09 19:50:33 EDT 2012 | action_101

Hello, We're building some boards with 01005's and the only issue we are running into is the solder is not reflowing. It's the damnest thing, we are having no issues with the printing process or placing the components, the two areas we thought we wo

01005 components and reflow profiles

Electronics Forum | Mon Apr 09 21:20:59 EDT 2012 | action_101

Interesting thought. Our paste is 89.2% according to the data sheet I have, but it still might be worth trying the 84-86% syringe blend. Thanks for the suggestion.

01005 components and reflow profiles

Electronics Forum | Fri Apr 13 16:52:07 EDT 2012 | hegemon

Hey Frazzled, you mean you don't prefer the back and forth flaming wars when someone disagrees with an opinion? How about "Agree" & "Disagree" for starters. Later we can add "YGTBK"(you got to be kidding), and "WP" (Wrong Planet) Great idea Frazz

01005 components and reflow profiles

Electronics Forum | Mon Apr 09 21:09:29 EDT 2012 | isd_jwendell

I haven't worked with anything as small as 01005s, but something you didn't mention is the %metal of your paste. I just switch from 90% to 89.5% (AIM NC257-2) and could tell the difference. Just an idea...

01005 components and reflow profiles

Electronics Forum | Fri Apr 13 12:31:23 EDT 2012 | markhoch

*Like* (There should be a way to "Like" or "Dislike" replies so that other Engineers can agree or disagree with a response. Doens't this sound like a good idea?)

01005 components and reflow profiles

Electronics Forum | Mon Apr 16 18:53:14 EDT 2012 | action_101

What is that garbage. How about you add flamer to like and dislike. I would have used it at least 3 times in this thread alone.

  1 2 3 4 5 6 7 8 9 10 Next

enig and reflow and profile searches for Companies, Equipment, Machines, Suppliers & Information

Best SMT Reflow Oven

World's Best Reflow Oven Customizable for Unique Applications
Selective soldering solutions with Jade soldering machine

Training online, at your facility, or at one of our worldwide training centers"
2024 Eptac IPC Certification Training Schedule

High Throughput Reflow Oven
PCB Depanelizers

Thermal Transfer Materials.