Electronics Forum | Wed Jun 16 14:05:23 EDT 1999 | Dave F
| A potential customer of our is inquiring if we have capability | for Hot Bar manufacturing in the PCBA manufacturing world. If someone can explain to me what this entails, I would greatly appreciate it. Thank you. | Gary: Tell your customer NO
Electronics Forum | Mon Jun 07 11:21:38 EDT 1999 | Brian Wycoff
| | I need to perform shear tests on components that have been glued prior to wave soldering. Can any one recommend a shear tester and some standardized info on testing? We have had problems with poor glue bonds and would like to implement a test m
Electronics Forum | Tue Jun 01 15:09:58 EDT 1999 | Tony
| Dear All, | | We are a medium sized sub contract manufacturing house, engaged in high mix, medium volume production. We are using no clean as well as Aqueous cleaning process. we are planning to buy a new wave soldering machine out of the follow
Electronics Forum | Wed Jun 02 04:04:58 EDT 1999 | Vinesh Gandhi
| | Dear All, | | | | We are a medium sized sub contract manufacturing house, engaged in high mix, medium volume production. We are using no clean as well as Aqueous cleaning process. we are planning to buy a new wave soldering machine out of the
Electronics Forum | Wed Jun 02 19:31:01 EDT 1999 | Tony
| | | Dear All, | | | | | | We are a medium sized sub contract manufacturing house, engaged in high mix, medium volume production. We are using no clean as well as Aqueous cleaning process. we are planning to buy a new wave soldering machine out o
Electronics Forum | Mon Jun 07 11:25:41 EDT 1999 | Brian Wycoff
| | | I have difficulty to convince my management to air-condition our manufacturing facilities. The room temperature fluxuates from 8 deg.C in the morning to 25 deg. C in the afternoon. The PCB topside temperatures in the reflow oven and wave solder
Electronics Forum | Mon Jun 07 16:52:51 EDT 1999 | Dave F
| | | | I have difficulty to convince my management to air-condition our manufacturing facilities. The room temperature fluxuates from 8 deg.C in the morning to 25 deg. C in the afternoon. The PCB topside temperatures in the reflow oven and wave sold
Electronics Forum | Fri May 28 07:37:52 EDT 1999 | Steve Cheung
Yes l know this problem keeps cropping up on the forum but l've missed some of the follow-ups. Our problem is that the lifting only occurs on 3% of production so actually detecting an improvement is difficult. We're actually having to inspect 144 p
Electronics Forum | Mon May 10 13:55:22 EDT 1999 | Deon Nungaray
| Can anyone tell me what the recommended "typical" cooling rates are after reflow? Are the cooling rates considered as critical to control as the heating rates and why/why not? | I do not think there is a "typical" post reflow cooling rate out ther
Electronics Forum | Thu Apr 29 20:03:10 EDT 1999 | Cunli Jia @ SMTnet
Steve, Check out the SMTnet First Chapter Bookstore on this site. We carry several tapes and books that may be of interest to you. If you find what you need elsewhere, please let us know too, so that we can add them in our bookstore. Please fol