Electronics Forum | Mon Jul 31 14:51:31 EDT 2006 | bhu
Can anyone suggest a supplier for gold solution when replating gold fingers that had solder on them?
Electronics Forum | Tue Aug 01 08:43:20 EDT 2006 | russ
Try the circuit repair corporation www.circuitrepair.com
Electronics Forum | Tue Aug 01 07:40:11 EDT 2006 | davef
Check the fine SMTnet Archives, like: http://www.smtnet.com/forums/Index.cfm?CFApp=1&Message_ID=9250
Electronics Forum | Wed Aug 02 08:09:51 EDT 2006 | Steve Gregory
Go to: http://www.hunterproducts.com/micro-metallizer.htm It's great system and you don't ever have to worry about spilling the solution.
Electronics Forum | Fri Jan 22 09:20:29 EST 2010 | jrr3434
Is there anyway to get solder off gold fingers besides replating them?
Electronics Forum | Wed Aug 31 12:33:25 EDT 2005 | Jaya
I have expirence running,double sided Imm gold boards recently which ed up a lot of solderability issue. The Imm gold need to be slightly more control during reflow oven area on it's profile.
Electronics Forum | Fri Aug 26 09:48:11 EDT 2005 | David
I have heard that there are problems using immersion gold on PCBs when working with BGAs. Is this correct? Is white tin more suitable?
Electronics Forum | Fri Aug 26 09:57:21 EDT 2005 | russ
The Immersion gold is not a problem with BGAs specifically but "black pad" which can be present anywhere. The unfortunate thing with BGAs is you cannot see it. Personally I hate white tin. It is okay for single sided boards running no-clean, but c
Electronics Forum | Fri Aug 26 14:15:16 EDT 2005 | David
Where could I find more information regarding the double sided reflow and flux problems with white tin?
Electronics Forum | Tue Sep 06 09:30:34 EDT 2005 | russ
I read it in Florida Cir-teks own literature. http://www.florida cirtek.com