Electronics Forum: gold thickness (Page 1 of 31)

Gold plating thickness on gold finger

Electronics Forum | Thu Oct 07 20:34:48 EDT 1999 | Tony Huang

Hi, Does anybody know what is the minimum gold plating thickness on the PCB goldfinger required by the industrial specifications - IPC, Bellcore, etc. Where can I find the information? Appreciate for the help! Thanks, Tony

Re: Gold plating thickness on gold finger

Electronics Forum | Fri Oct 08 17:12:31 EDT 1999 | Dave F

| Hi, | | Does anybody know what is the minimum gold plating thickness on the PCB goldfinger required by the industrial specifications - IPC, Bellcore, etc. Where can I find the information? Appreciate for the help! | | Thanks, | Tony | Hi Tony:

Gold thickness

Electronics Forum | Thu Jul 10 09:16:41 EDT 2008 | aj

Hi all, What should the typical gold thickness be on ENIG boards ? aj...

Gold thickness

Electronics Forum | Fri Jul 11 08:17:22 EDT 2008 | aj

Hi Dave, Yes that is correct. I had a XRF carried out on some boards that I am having solderability issues on and the report came back with 0.04um - 0.05um as the measured gold thickness. Previous batches that went through fine measured 0.07-0.11u

Gold thickness

Electronics Forum | Tue Jul 15 16:30:57 EDT 2008 | boardhouse

Hi Aj, Recommended Immersion gold thickness would be 3-5 Micro inches over 140 -200 micro inches of Nickel. Thicker Immersion gold than 5 micro inches can cause solder joint embrittlement. Gold readily dissolves in molten solder and will be present

Gold thickness

Electronics Forum | Mon Jul 28 06:23:29 EDT 2008 | cobar

Please look up http://www.shanelo.co.za/Black%20Pad%20Index.htm and check out the article named"Soldering to gold a practical guide."

Gold thickness

Electronics Forum | Thu Jul 10 22:19:14 EDT 2008 | davef

Search the fine SMTnet Archives to find threads like: http://www.smtnet.com/forums/Index.cfm?CFApp=1&Message_ID=33661

Gold thickness

Electronics Forum | Fri Jul 11 02:42:40 EDT 2008 | aj

Thanks Dave, IPC-6012 states min at 0.05um. Has this been a update or is it for a different class? thanks, aj...

Gold thickness

Electronics Forum | Fri Jul 11 07:04:26 EDT 2008 | davef

2 uinch, right? Here is the revision level for IPC documents: http://www.ipc.org/4.0_knowledge/4.1_Standards/revstat1.htm

soft gold vs immersion gold

Electronics Forum | Wed Aug 11 16:09:50 EDT 2004 | Kris

Hi How does one distinquish between hard gold and immersion gold ? thickness is 4 to 10 u" for Au and 300 to 400 u" for nickel what happens if the gold drops below 3" and the nickel is above 350" what are the typical failure modes associated with

  1 2 3 4 5 6 7 8 9 10 Next

gold thickness searches for Companies, Equipment, Machines, Suppliers & Information

Best SMT Reflow Oven

World's Best Reflow Oven Customizable for Unique Applications
consignment program

Nozzles, Feeders, Spare Parts - Siemens, Fuji, Juki, Yamaha, etc...
2024 Eptac IPC Certification Training Schedule

High Throughput Reflow Oven
design with ease with Win Source obselete parts and supplies

"回流焊炉"