Electronics Forum | Wed Oct 18 09:44:38 EDT 2000 | mike weekes
we're considering PWB finishes other than HASL - the uneven plating contributed to defects and the residues exceed our goal for PWB cleanliness. What success have any of you had with CuOSP, Immersion Silver, Gold or other finishes? Did you have to
Electronics Forum | Thu Aug 31 21:15:46 EDT 2000 | Dave F
From the SMTnet Library try: http://www.merix.com/resourcecntr/papers/osp.doc http://www.merix.com/resourcecntr/papers/hasl_alt.doc http://www.itm-smt.com/articles.html * "Organic Solderability Preservatives" * "OSPs - Better Living Through Modern Ch
Electronics Forum | Thu Aug 06 03:57:59 EDT 1998 | STONEY TSAI
Hi, friends, The gold plating and HASL boards made some difference on solderability for both reflow and wave soldering processes. It is difficult to investigate the interactions between raw materials and process parameters setting. Anyone provides th
Electronics Forum | Wed Jul 29 13:44:45 EDT 1998 | David Spilker
We are investigating alternatives to HASL finishes for more dense PWBs. OSP is not a good choice because of low solid flux and possibly long shelf life. Immersion gold is expensive and so far has been more difficult to wave solder. Has anyone had
Electronics Forum | Wed Jun 10 14:00:16 EDT 1998 | Jason Gregory
Okay, here's a stupid question. What exactly is HASL and OSP? We are going to delve into this technology where I work and I want to utilize the wealth of knowledge here to make life easier. Specifically, what are the differences, the advantages, disa
Electronics Forum | Wed Jun 10 13:59:41 EDT 1998 | Jason Gregory
Okay, here's a stupid question. What exactly is HASL and OSP? We are going to delve into this technology where I work and I want to utilize the wealth of knowledge here to make life easier. Specifically, what are the differences, the advantages, disa
Electronics Forum | Mon May 18 13:18:25 EDT 1998 | Chrys
I'm reviewing my board fab spec. It calls for a minimum SnPb thickness of 50 microinches on HASL PWB's. I've looked at other specs that call out anything from 30 to 80 microinches, and others that just say the copper pad must be covered and soldera
Electronics Forum | Tue Mar 24 09:50:45 EST 1998 | Justin Medernach
| Do I need to specify any type of special | finishing to my PCB manufacturer when having | boards fabbed that contain BGA footprints ??? | Thanks, | Stuart No special finish is required. I have assembled boards with BGA population that had HASL,
Electronics Forum | Thu Feb 19 12:32:25 EST 1998 | Earl Moon
| We are currently investigating alternatives to HASL for circuit boards with 20 mil pitch smt pads and below. If you have experience with this product or simular immersion tin products with respect to manufacturing or assembly I am very interested
Electronics Forum | Thu Feb 19 12:35:13 EST 1998 | Earl Moon
| | We are currently investigating alternatives to HASL for circuit boards with 20 mil pitch smt pads and below. If you have experience with this product or simular immersion tin products with respect to manufacturing or assembly I am very interest