Electronics Forum | Wed Oct 10 16:16:15 EDT 2001 | lisa
Hello all, I'm looking for some advice on inter-metallic formation. I have some circuit board finished with Immersion Tin, Immersion Silver and OSP. They have been reflowed with solder past and components,the joints look good. What can I expect fo
Electronics Forum | Tue Oct 16 11:25:29 EDT 2001 | stepheno
Don't overlook tools and equipment suppliers and their sales staff. I plan on having an ESD audit done by one of our tool suppliers. I know they will come in and say here are your problems and here are products we sell that will fix them. On the o
Electronics Forum | Tue Oct 16 11:51:26 EDT 2001 | bobm
i am using the epibond. i had alpha come in and look at our set up. they told me that the epibond can be reflowed at regular temp profiles with no problems. because i only have one oven and two pick n place machines it was important to be able to run
Electronics Forum | Mon Oct 22 17:47:47 EDT 2001 | davef
We on SMTnet have danced around this component package, but there is not a "background" of knowledge in the fine SMTnet Archives. We in our company use this component package, but have not seen the problems you discuss. [We see other problems.] Th
Electronics Forum | Wed Oct 24 02:19:34 EDT 2001 | Leo Gapasin
We have been monitoring our solder defects at post-SMT, post-Wave, etc.in our plant. I want to compare our process performance to a "bench mark" for solder defects at post-SMT. The question I have is what is the "bench mark" for soldering defects in
Electronics Forum | Wed Nov 07 08:06:29 EST 2001 | hany_khoga
Dear All : 1- We assemble mixed technology boards. For some reasons, sometimes we store them semi assembled (only SMT). Knowing that they have plastic BGA,s , can the wave solder m/c affect or damage those BGA,S on continuation their production?
Electronics Forum | Mon Sep 16 13:04:19 EDT 2002 | dragonslayr
JoJo- please keep your "mining" for leads to other forums; you have activated a nearly one year old thread that has no relevance today other than your interest in your making a contact. Try contacting the original poster direct. If you have somethin
Electronics Forum | Tue Nov 20 04:38:18 EST 2001 | frha
How to implement an easy SPC in the production line? Im looking for relevant characteristics to perform SPC on electronics (e.g. PC-module with motherboard and UPS, power supply's, field bus cards, servo drive systems etc). I understand that compon
Electronics Forum | Thu Dec 06 10:10:52 EST 2001 | edmentzer
We have a MY12 with the Hydra head, its a great machine for us. We had a MultiTroniKs before. The MYDATA is easy to program, easy to use, is very accurate, is easy to change from job to job. In the 18 months we have had the machine the only proble
Electronics Forum | Fri Dec 07 09:43:04 EST 2001 | Russ Steiner
I have a mixed technology PCB that has SMT all on bottom, TH parts on both sides (Yes, I realize that's bad. Can't be avoided.) We have designed a 10-up panel, 2 x 5 array. There are 50 leads per bd, 500 per panel. How much time is reasonable to a