Electronics Forum | Wed Mar 30 17:32:55 EDT 2011 | gaz
Hi, We are using ws488 sn100c paste. Anyone have a profile for a 5 zone oven that has worked well for you?
Electronics Forum | Thu Mar 31 10:22:57 EDT 2011 | swag
We are going to buy a new reflow oven. I'm currently comparing Rehm VXS3150 and Heller 1809 Mark III. Both should meet our needs as far as zones. Does anyone have experience to share for either? Good service from these companies?
Electronics Forum | Fri Apr 01 10:12:41 EDT 2011 | babe7362000
Does anyone else use splice tape on Juki feeders? If so what kind of splice and what kind of tape is being used to connect them? Thanks for any input.
Electronics Forum | Mon Apr 04 11:46:20 EDT 2011 | frcdave
I was thinking the same thing. Try turning off your anchors and look at the size of your search and % match you have set. if you are concerned about not catching missing components, try training a negative template.
Electronics Forum | Thu Apr 07 13:57:39 EDT 2011 | remullis
Thanks Graham that's what I'm thinking. I'm gonna have to steal this oven for a while. Thanks again.
Electronics Forum | Wed Apr 06 12:21:14 EDT 2011 | ripper
Hi, I am process engineer in PCBA factory.I have a question about gold plating on BGA.I want to know difference soldering performance between gold plating electrolytic and ENIG.Many thank for any idea.
Electronics Forum | Mon Apr 11 00:05:54 EDT 2011 | vinitverma
PROCAM is intended to extract Centroid from the raw Gerber only. You just need to have 2 layers (paste or mask layer - to identify pads, and silk layer - for reference designators). Centroid is the output of PROCAM.
Electronics Forum | Wed Apr 13 09:15:07 EDT 2011 | blnorman
Have used IC for years, but I'm not familiar with that, ROSE maybe. Its a stretch, but maybe R/O/I would be rosin/resin, organic, or inorganic for the type flux being used?
Electronics Forum | Fri Apr 15 18:41:35 EDT 2011 | swarnergictg
We had a similar problem with contaminated leads that was rectified by having a company strip the existing finish and re-tin the leads. After the procedure the leads accepted solder with no issues.
Electronics Forum | Tue May 03 21:20:58 EDT 2011 | littlebone
Exactly. And now a day, we are sourcing quite a number of alternative component. (e.g. IC, capacitor...) Template matching may took long time to calibrate the variances too. Desperate to look for cyberoptics representative to have a presentation