Electronics Forum | Tue Dec 19 16:26:24 EST 2006 | samir
Grant, Newer lead-free fluxes have 6%-10% solids content - more activator, therefore leave more "visible" residues. Old technology tin-lead fluxes got down to as low as around the 4%-6% range (I'm going off memory, so me might be wrong)... You'll
1 |