Bubbles on solder joint(after conformal coating curing)

Electronics Forum | Mon Dec 28 09:12:56 EST 2009 | kpm135

@tommyg_fla According to the TDS the recommended coating thickness for Humiseal 1B31 is only 1-3 mils so if I had to guess I would say your issue might be that you're re-coating over the first pass too soon. All the solvent hasn't evaporated and the