Electronics Forum | Thu Apr 26 12:03:30 EDT 2001 | Steve
IPC has some good publications that would also help, such as IPC-S-816. (ipc.org) Subscribe to SMT magazine. I have gained a ton of knowledge from their articles. (smtmag.com) Good luck.
Electronics Forum | Tue Feb 25 13:54:09 EST 2003 | slthomas
This might be a little more that you've bargained for, but have you had a look at IPC-S-816? Obviously it needs to be tailored to your process, your quality needs, etc.
Electronics Forum | Wed Aug 04 15:27:03 EDT 2004 | Rush Fan
I might suggest that you check with your solder paste manufacturer to see what is recommended for time over reflow. Typically, I think most are between 60 and 90 seconds over 183. Also, consider the rate of cooling. The faster you cool the solder, th