Electronics Forum: ipc-tm-650

force between the pad and laminate material

Electronics Forum | Wed Jun 12 08:13:29 EDT 2002 | davef

Don't sound proper. There is no specification. Pad peel strength test methods are: * IPC-TM-650, Method 2.4.21 for multiple solderings * IPC-TM-650, Method 2.4.8 for copper peel with a Instron machine. Typical requirement for Cu is: 6 lbf/in [1

CCGA and overprinting?

Electronics Forum | Mon Oct 15 12:42:36 EDT 2001 | davef

I hate getting "roped" into math stuff, but here I go again ... Area of aperture = volume of paste / stencil thickness = {[5000 mil^3] / 5 mil} = 1000 mil^2 Side of the square aperture = Sqrt of the area = [1000 mil^2]^1/2 = 32 mil Diameter of ape

Re: MoonMan and Tetras

Electronics Forum | Tue Apr 27 05:26:14 EDT 1999 | Charles Stringer

| | Hey MoonMan, | | | | Did I catch in one of your fabulous threads that you're using Tetra stencils? I'm anxious to find out how you're liking them. | | | | We we're all set up to go to Tetras, then mgt decided to close down our factory - Dooop!

Re: MoonMan and Tetras

Electronics Forum | Tue Apr 27 09:26:43 EDT 1999 | Chrys Shea

| | | Hey MoonMan, | | | | | | Did I catch in one of your fabulous threads that you're using Tetra stencils? I'm anxious to find out how you're liking them. | | | | | | We we're all set up to go to Tetras, then mgt decided to close down our factor

Re: PCB fab supplier supplier/evaluation

Electronics Forum | Sun Aug 08 11:15:32 EDT 1999 | Earl Moon

| | Mike, | | | | Got your message and those of others concerning PCB fab supplier evaluation and qualification check lists, etc. I have a severe problem here in WI as I can hardly access the internet, and when I do it is cut off abruptly for no goo

Discoloring of Soldermask and silkscreen

Electronics Forum | Mon Apr 12 19:28:26 EDT 1999 | Tom B

Netters, When I reflow a PCB there is a discoloration of silkscreen and mask. It appears if Profile is too hot! But I dont think so, maybe I'm wrong? 1. Kester 293 no clean 2. 2.1 C/s for 30s to 150 C 3. .5 - .7 C/s for 60s to 185 C 4. 1.5 C/s u

Foam fluxer maintenance, storage and cleaning

Electronics Forum | Sun Nov 08 15:27:25 EST 2015 | davef

Thinner: Flux thinner, NOT paint thinner We kept a spare stone in thinner in inventory. We cut PVC pipe to size, cap in one end, screw thread on the other, stone inside, filled with flux thinner and covered with a screw cap. I don't remember who we

Re: Discoloring of Soldermask and silkscreen

Electronics Forum | Tue Apr 13 18:11:00 EDT 1999 | Jimmy Strain

| Netters, | | When I reflow a PCB there is a discoloration of silkscreen and mask. It appears if Profile is too hot! But I dont think so, maybe I'm wrong? | | 1. Kester 293 no clean | 2. 2.1 C/s for 30s to 150 C | 3. .5 - .7 C/s for 60s to 185

Re: Discoloring of Soldermask and silkscreen

Electronics Forum | Mon Apr 19 11:21:03 EDT 1999 | Travson

| Netters, | | When I reflow a PCB there is a discoloration of silkscreen and mask. It appears if Profile is too hot! But I dont think so, maybe I'm wrong? | | 1. Kester 293 no clean | 2. 2.1 C/s for 30s to 150 C | 3. .5 - .7 C/s for 60s to 185

Re: Discoloring of Soldermask and silkscreen

Electronics Forum | Mon Apr 19 20:49:13 EDT 1999 | Dave F

| Netters, | | When I reflow a PCB there is a discoloration of silkscreen and mask. It appears if Profile is too hot! But I dont think so, maybe I'm wrong? | | 1. Kester 293 no clean | 2. 2.1 C/s for 30s to 150 C | 3. .5 - .7 C/s for 60s to 185

  1 2 Next

ipc-tm-650,method and 2.1 searches for Companies, Equipment, Machines, Suppliers & Information

Reflow Oven

IPC Certification Training from the comfort of your home or office
FPC* - Fluid Pressure Control - Dispensing Pump

Training online, at your facility, or at one of our worldwide training centers"
PCB Handling with CE

MSD Dry Cabinets
PCB Handling Machine with CE

High Speed Precision In-Line SPI System - Mirtec MS-11