Electronics Forum | Thu Jun 25 22:25:24 EDT 2009 | boardhouse
In the life of this product that you have been doing this process, has the material alway's been IT180 material? One problem with Lead free material is that it is more fragile that standard FR4 Epoxy laminate. And is known to have chipping or fractu
Electronics Forum | Wed Jul 01 13:17:39 EDT 2015 | davef
Cheryl Tulkoff and Randy Schueller do a good job summarizing the thinks on pad cratering here: http://www.smta.org/chapters/files/uppermidwest_padcratering.pdf Potential Mitigations to Pad Cratering * Board Redesign * Solder mask defined vs. non-s
Electronics Forum | Mon Jun 11 21:56:41 EDT 2001 | davef
Continuing, I�ve optioned about the uselessness of shear testing of solder connections on this forum previously. So, the points that you make about the elusiveness of developing a standard for measuring solder connection strength is well taken. I�l