Electronics Forum | Wed Aug 04 16:49:24 EDT 2004 | jim_bob
Regarding Lead Free component finishes, vendors are zeroing in on matte tin plating as the finish of choice. What test are performed, to determine if a finish is "matte" type (vs. non-matte)?
Electronics Forum | Mon Jun 29 19:02:49 EDT 2009 | davef
Current limiting resistor: Personel safety Electrical equipment on the ESD matt: We need more information. Is the equipment ground of the equipment in contact with the matt? Or are the insulating pads on the bottom of the equipment in contact with t
Electronics Forum | Mon Oct 24 17:56:57 EDT 2005 | Ali
Hello all: A couple of queries on matte Sn plating: My Application: 2 Reflows in subassembly reflow+ 8 Hr Steam age+ Solderability (Dip and look) for sub assembly to mother board soldering. Queries on Matte Sn: 1- Different plating vendor
Electronics Forum | Mon Nov 07 17:24:15 EST 2005 | Ali
Hi Dave, I am working on electroplated matte Sn.
Electronics Forum | Wed Nov 07 06:33:21 EST 2007 | chineechooze
MATT MATT
Electronics Forum | Tue May 16 16:36:18 EDT 2006 | dougm
Has anyone had issues with chips not making a reliable connection in sockets with a matte tin finish (RoHS compatible)? We have had issues with these types of sockets. I sent some to the manufacturer, and was told there weren't any problems. We re
Electronics Forum | Mon Oct 11 13:08:29 EDT 1999 | Dave F
| Folk's, | | I'm just tying up some loose end's on my Master's Thesis on solderballing @ wave soldering and the effect the topography of the mask / PCB has on it. | I was wanting to do a straw poll on you guy's as to the type of resist's you are us
Electronics Forum | Mon Jul 10 09:23:47 EDT 2006 | Rob
Hi Dougs, Info as follows: TAICOM TSD42: Matte Tin, 240C for 5 secs TAICOM TSD08: Matte Tin, 225/3 secs (I wouldn't!) TAICOM TKB06MSL: Matte Tin 260/40 secs (TBC) HARTING 09232486824: Harting don't supply. TAICOM TI40BHS: Matte Tin, 225/3 secs (I
Electronics Forum | Wed Nov 13 18:00:59 EST 2013 | davef
It's too bad that SMTnet won't let us view your pdf. I asked the geeks to fix that. If someone really want to read it Matt can likely get it off to you. Is it OK to do that, Matt? Anyhow, the Trace Labs report seems to be focused on some SMT pad dis
Electronics Forum | Thu Oct 24 04:42:39 EDT 2024 | asyraafzai96
Hi, I am facing tiny solder ball issue and flux stain all around the PCB. For info this is my first time run the PCB with matte finishing. I don't have any issue with the glossy finish PCB. For more info I use all the same setting between gloss and m