Electronics Forum | Fri Nov 08 16:47:55 EST 2019 | solderingpro
I work with PROMATION USA and we offer solutions for large magazine handling (specifically for LED Mfg.). Please refer to image below to assist with your request for info: https://images.app.goo.gl/ozvTXM4JgyjoXaSM9
Electronics Forum | Fri Feb 05 12:33:21 EST 2021 | dontfeedphils
In a past life I worked at a CM that used MFG P/Ns and the only thing I had to watch out for was character limits in the P/N field for the machines as well as special characters the machine couldn't handle.
Electronics Forum | Mon Aug 14 13:51:37 EDT 2023 | calebcsmt
I'm actually currently in the process of discussing with stencil MFG regarding the apertures and reduction to see if perhaps it was not optimal for this fine pitch QFN, as just as you mentioned, we have similar products with similar QFNs that do not
Electronics Forum | Tue Mar 19 14:12:59 EDT 2024 | jergod
We have different codes for different mfg's. Also we try to stay away from text inspection as much as possible since that is done already in incoming inspection.
Electronics Forum | Wed Mar 27 02:36:27 EDT 2024 | dekhead
DEK 265LT was not mfg until 1995/6, verify model; what camera (4 possibilities on LT) is on machine? Have you verified / replaced video cable from camera all the way back to cognex?
Electronics Forum | Fri Jun 11 18:36:57 EDT 2004 | russ
No Rob you didn't misunderstand, I forgot the decimal point! Lets try this .2" thick (I have built this and yes it was V-Scored) We didn't break any caps on that baby just fingers, that was the wildest VScore job I have ever seen I don't know how the
Electronics Forum | Thu Sep 11 11:45:33 EDT 2008 | swag
Never did find a fool proof solution. Solderability seemed O.K. (at least using the methods we have available in house). Tinned parts and placed by hand and saw little improvement. Pad design is slightly different than recommended but likely not i
Electronics Forum | Thu Oct 01 07:09:53 EDT 2009 | g2garyg2
Good Morning Here are a few thoughts. When mfg large flex circuits you will need to fixture them to create a stable production environment. As such, the foot print fo the product grows. So you may require systems that can handle 20 inch width by 38 i
Electronics Forum | Tue Mar 23 15:46:28 EDT 2010 | pilusa
The AIM flux is for the process and not for the tip tinning. The flux I was referring to is what is used to keep the tip wetted which was one of your original problems. Regarding the process, in my experience the AIM flux is not very active and there
Electronics Forum | Fri Feb 11 05:44:08 EST 2000 | Dean
Sounds like black pad to me. I just suffered this last week. Track your fab lot codes. Just in case. I processed 1000 fabs of 2 lot codes through 1 line (also WS609). 1 lot code failed with black pad the other did not. With one common mfg. proc