Electronics Forum | Sun Apr 25 17:30:25 EDT 1999 | Mohammad Yunus
| | | | We are just starting to manufacture a PCB with a .039" fine-line PBGA. We are currently seeing voids, mainly in the center, that are as much as 45%. We also intermittently see the corner balls of the PBGA smaller than the center balls. We are
Electronics Forum | Tue May 26 20:18:09 EDT 1998 | Justin Medernach
| | | | I'm reviewing my board fab spec. It calls for a minimum SnPb thickness of 50 microinches on HASL PWB's. I've looked at other specs that call out anything from 30 to 80 microinches, and others that just say the copper pad must be covered and
Electronics Forum | Tue May 26 21:27:33 EDT 1998 | Earl Moon
| | | | | I'm reviewing my board fab spec. It calls for a minimum SnPb thickness of 50 microinches on HASL PWB's. I've looked at other specs that call out anything from 30 to 80 microinches, and others that just say the copper pad must be covered a
Electronics Forum | Wed May 27 11:19:34 EDT 1998 | Earl Moon
| | | | | | I'm reviewing my board fab spec. It calls for a minimum SnPb thickness of 50 microinches on HASL PWB's. I've looked at other specs that call out anything from 30 to 80 microinches, and others that just say the copper pad must be covered
Electronics Forum | Wed Jan 11 22:47:31 EST 2006 | davef
We didn't intend to light anyone's fur on fire [get anyone's underwear in a knot, roil the waters, have a cow man] about consultants. The Phil Zarrow wrote a useful paper that could help in evaluating paste. Here read it ... Evaluating Solder Paste
Electronics Forum | Thu May 26 08:52:42 EDT 2011 | davef
Phil Zarrow wrote a useful paper that could help in evaluating paste. Here read it ... Evaluating Solder Paste � Not An Option Contributed by Phil Zarrow of ITM an Independent SMT consulting firm With soldering being the dominant source of assembly