Electronics Forum | Mon Sep 28 19:07:47 EDT 1998 | Steve Gregory
| I have had some field failures returned recently, the boards had flux contamination under the components in a sensitive area, Nothing really visible until the component was removed, and the board had no evidence of rework of any type. Is it poss
Electronics Forum | Fri Sep 04 09:33:40 EDT 1998 | Stefan W.
| I need advice for locating 23 Gull wing LED's (all in a straight line) in the x,y, and z axis for a SMT PCB. It is a Hewlett Packard LED (P/N HMLA-QH00-01). The application uses a CCD to detect the position of a ball which floats in a resevior fo
Electronics Forum | Fri Aug 21 07:57:20 EDT 1998 | Earl Moon
| | | Will somebody please explain HASL (here). Thanks. | | Tryin: HASL: Hot Air Solder Leveled. A board fabrication process that applies an oxidation preventing solder coating to copper pads on the board. Dave F | You do this to keep the green s
Electronics Forum | Fri Jun 19 14:25:24 EDT 1998 | Earl Moon
| | Has anyone had experience with placing BGA on gold plated boards. I thought I read a while ago there was a problem with embrittlment causing cracked joints. If anyone has experience with this your feedback would be great. | | Mike | There has b
Electronics Forum | Fri May 29 13:42:34 EDT 1998 | Steve Gregory
Hi Jason! I can probably find something documented for you, but the easiest way to convince your QA people is just to show them. If you have a board around that has some 1206 locations all in a row, print the board with paste and then plac
Electronics Forum | Fri May 29 16:12:11 EDT 1998 | Jason Gregory
| Hi Jason! | I can probably find something documented for you, but the easiest way to convince your QA people is just to show them. | If you have a board around that has some 1206 locations all in a row, print the board with paste and the
Electronics Forum | Tue May 26 21:27:33 EDT 1998 | Earl Moon
| | | | | I'm reviewing my board fab spec. It calls for a minimum SnPb thickness of 50 microinches on HASL PWB's. I've looked at other specs that call out anything from 30 to 80 microinches, and others that just say the copper pad must be covered a
Electronics Forum | Wed May 27 11:19:34 EDT 1998 | Earl Moon
| | | | | | I'm reviewing my board fab spec. It calls for a minimum SnPb thickness of 50 microinches on HASL PWB's. I've looked at other specs that call out anything from 30 to 80 microinches, and others that just say the copper pad must be covered
Electronics Forum | Fri May 08 18:39:17 EDT 1998 | Steve Gregory
| | As usual, we are faced with too many components and not enough board on a new design. Does anyone have experience wavesoldering .025" pitch TSOPs on the bottom side? | | Any advice is appreciated. | | Greg Hi there Greg! First, I just gotta
Electronics Forum | Mon Mar 09 16:36:38 EST 1998 | Jim McLenaghan
| We have a double sided pcb that is surface mount on both sides. Now a Through Hole connector has been added. Appart from hand soldering does anyone have info. on reflow soldering the part. The connector is 0.1mm pitch, square legs. | 1) Do you need