Electronics Forum | Mon Nov 12 16:14:47 EST 2001 | davef
Yes!!! How can we assemble boards with 20 pitch when we allow 0.008� error to the master art? Excellent question!!! IPC-D-300G has nothing to do with assembler requirements. It is written by and for fabricators, so that they can be comfortable.
Electronics Forum | Thu Mar 28 15:53:49 EDT 2019 | SMTA-Jon
As a CM, we don’t have a lot of input on the PCB layouts we receive. Some engineers/software packages output the paste layer 1 to 1, some do an across the board reduction, and some set each part up individually with different reductions per footprin
Electronics Forum | Wed Aug 19 12:20:24 EDT 1998 | MARK J.
| Hi there, | I'm actually facing a lot of trouble with PCB's presenting up to 3mm of bow /twist at reception i.e. before assembly. The PCB size is 220 by 230mm. The boards are to be assembeled SMD double sides with 05.mm pitch on both sides. In orde
Electronics Forum | Mon Dec 16 19:05:57 EST 2002 | davidduke
Steve , I agree with all the responses you have received. Randy Villeneuve is absolutly correct in all of his assesments and I would consider him an expert with the process , Gris is correct about adding a "heat sink" to the process complicating pr
Electronics Forum | Wed Aug 19 08:00:55 EDT 1998 | Earl Moon
| Hi there, | I'm actually facing a lot of trouble with PCB's presenting up to 3mm of bow /twist at reception i.e. before assembly. The PCB size is 220 by 230mm. The boards are to be assembeled SMD double sides with 05.mm pitch on both sides. In orde
Electronics Forum | Fri Feb 28 09:08:03 EST 2003 | davef
Without drilling through the numbers, they're probably correct. Recognize that standard warp / twist specs [IPC-A-610 1.5% for PTH only and 0.75% for SMT] are not going to make it on tech boards. You need to define specific requirements. This warp
Electronics Forum | Mon May 12 15:13:29 EDT 2014 | emeto
Thank you guys. As we are speaking I keep examine the problem and here is what I got so far. 1. I measured the temperatures on my profile and the lead is hotter than the board. The lead goes 12 seconds earlier than the pad and is taking the solder.
1 |
Products, services, training, and consulting for the assembly, rework & repair of electronic assemblies. BGA process experts. Manufacturers Rep & Sole Agent in North America for Shuttle Star BGA Rework Stations.
Training Provider / Manufacturer's Representative / Equipment Dealer / Broker / Auctions / Consultant / Service Provider
1750 Mitchell Ave.
Oroville, CA USA
Phone: (888) 406-2830