Desiccants and pcb finish degradation?

Electronics Forum | Tue May 15 15:15:53 EDT 2001 | ohboy

Hi all, I just discovered this forum and I'm very impressed. We have a vendor who recently stopped placing desiccants in the vacuum packaging for our pcbs. (Yes, it's on the dwg!) His reasoning was that the desiccants can degrade the finish on the

Desiccants and pcb finish degradation?

Electronics Forum | Wed May 16 08:48:12 EDT 2001 | ohboy

I been a bunch o' places...! Some good, some bad, re-inventing the wheel in many cases. Our specs are pretty specific in a lot of cases, but that doesn't mean they always get followed. It usually becomes a case of "It's not quite right, but we rea

The minimal distance btw component and the edge of pcb

Electronics Forum | Tue Nov 01 12:28:36 EDT 2016 | comatose

It depends. Are you hand breaking them, rotary knife or linear knife? Hand break you want to be about 5mm (and it isn't a great practice even then) with a rotart knife you want to keep parts probably 3mm, especially capacitors. With a linear knife we

Cleaning Machine and Chemistry

Electronics Forum | Mon Feb 19 11:36:39 EST 2001 | billschreiber

Hello Mark, I wish it were that simple so I could direct you to a particular manufacturer and stencil cleaner model. Unfortunately, there are several issues complicating the process of cleaning all these applications in one machine. First and fore

0402's and Gluing.............

Electronics Forum | Thu Feb 10 09:01:40 EST 2005 | russ

I have done that also, It does work well. One issue we had was that the mask didn't come right off during the first wash cycle since it was put on much heavier than the mfgr suggested (.01"). We had to soak them in some water first to soften it up

0402's and Gluing.............

Electronics Forum | Wed Feb 09 21:19:03 EST 2005 | Mrduckmann2000

Russ, We can not use a wave pallet, already went that route. We have parts next to the thru-hole pins and between thru-hole pins. I am going to try an experiment in the next day or so with solder mask. I plan to solder SMT parts on the back of se

Flexi boards and uBGA

Electronics Forum | Thu Jul 06 12:06:12 EDT 2006 | pavel

Rob, do you have any tip on reliable supplier of "really flat" flexible pcb? We tried several but all with issues. Thank you. Pavel

Imm Silver and Voiding

Electronics Forum | Thu Jun 22 00:16:24 EDT 2006 | Gman

Hello, Has anyone had issues with voiding while using Imm Silver PCB finish. Does thickness of silver, contamination of the plating bath or other factors if you come point out cause voids due to the plating.

Headers and SMT

Electronics Forum | Tue Sep 29 10:53:42 EDT 2015 | marlyn

Hey there fellow people with SMT issues... What's the proper procedure for soldering through-hole headers on the back-side of the PCB (pins poking out on same side as SMT parts)? ( Yes - I did the SMT side first and am now faced with LOTS of pin-poin

LGA and Solderballs

Electronics Forum | Tue Nov 28 21:16:17 EST 2006 | davef

J Rose at EMPF says: The introduction of no-clean solder fluxes in electronics manufacturing has given rise to greater levels of solder balling simply because the opportunity to remove them in the wash process does not exist. They are typically cause

  1 2 3 4 5 6 7 8 9 10 Next

pcb and washing and issue searches for Companies, Equipment, Machines, Suppliers & Information

Precision PCB Services, Inc
Precision PCB Services, Inc

Products, services, training & consulting for the assembly, rework & repair of electronic assemblies. BGA process experts. Manufacturers Rep, Distributor & Service Provider for Seamark/Zhuomao and Shuttle Star BGA Rework Stations.

Training Provider / Manufacturer's Representative / Equipment Dealer / Broker / Auctions / Consultant / Service Provider

1750 Mitchell Ave.
Oroville, CA USA

Phone: (888) 406-2830