Electronics Forum | Thu Jun 04 14:30:13 EDT 1998 | Igmar
I would appreciate any information concerning the wash and bake of blank Printed Circuit Boards before assembly. + Is it necessary to wash and bake PCB�s before assembly? + If any, what is the reason for wash and bake of PCB�s? + If any, what type of
Electronics Forum | Thu Feb 12 16:50:40 EST 1998 | Igmar
I would appreciate any information concerning the wash and bake of blank Printed Circuit Boards before assembly. + Is it necessary to wash and bake PCB�s before assembly? + If any, what is the reason for wash and bake of PCB�s? + If any, what type of
Electronics Forum | Thu Feb 12 17:21:07 EST 1998 | Justin Medernach
| I would appreciate any information concerning the wash and bake of blank Printed Circuit Boards | before assembly. | + Is it necessary to wash and bake PCB�s before assembly? | + If any, what is the reason for wash and bake of PCB�s? | + If any, wh
Electronics Forum | Wed Jul 28 20:28:26 EDT 1999 | Carlos Palacios
Currently, we are baking any PCB before process on SMT, the 'reason' is to dry any possible humidity that could be inner the PCB, it does not matter if the PCB is multilayer or not. We bake PCB's at 107C for 4 hrs and the board must be process into n
Electronics Forum | Mon Oct 31 20:35:58 EST 2005 | milroyperera
If I brief shifting, I checked the component before it enter the reflow oven and saw that the IC is perfectly aligned on the pads but when it comes out from the oven the IC is floated on the pads. The floating is irregular and the IC is shifted away
Electronics Forum | Wed Jul 28 20:56:58 EDT 1999 | Dave F
| Currently, we are baking any PCB before process on SMT, the 'reason' is to dry any possible humidity that could be inner the PCB, it does not matter if the PCB is multilayer or not. We bake PCB's at 107C for 4 hrs and the board must be process into
Electronics Forum | Thu Jul 29 00:23:45 EDT 1999 | ScottM
| Currently, we are baking any PCB before process on SMT, the 'reason' is to dry any possible humidity that could be inner the PCB, it does not matter if the PCB is multilayer or not. We bake PCB's at 107C for 4 hrs and the board must be process into
Electronics Forum | Thu Jul 29 12:33:38 EDT 1999 | Wolfgang Busko
| Currently, we are baking any PCB before process on SMT, the 'reason' is to dry any possible humidity that could be inner the PCB, it does not matter if the PCB is multilayer or not. We bake PCB's at 107C for 4 hrs and the board must be process into
Electronics Forum | Tue Feb 17 15:24:17 EST 2009 | glynnhamer
I know this is going to sound rather sad, but we have been using a Capton tape for years that contains silicone to mask large components as they go over the wave, as well as large plated holes on the pcb. It was handed down for years as accepted prac
Electronics Forum | Tue Aug 25 09:47:32 EDT 1998 | Earl Moon
| Thanks for the great info, man!! | | | | | What conditions make Earl Moon say "damn, why can't XXX get the HASL right? Just look at this crummy board. Get a RMA No. Stat." | | I don't have to get that frustrated because I deal with those who do
Products, services, training & consulting for the assembly, rework & repair of electronic assemblies. BGA process experts. Manufacturers Rep, Distributor & Service Provider for Seamark/Zhuomao and Shuttle Star BGA Rework Stations.
Training Provider / Manufacturer's Representative / Equipment Dealer / Broker / Auctions / Consultant / Service Provider
1750 Mitchell Ave.
Oroville, CA USA
Phone: (888) 406-2830