Electronics Forum | Tue Aug 31 13:23:37 EDT 2004 | frankracine
Thanks Ken for your reply. Concerning OSP, there are a few negative points that I must considered for our application. I've read all the following points in an Entek document. Never test it. - If you have a miss print and you clean the PCB, the co
Electronics Forum | Wed Sep 01 09:29:03 EDT 2004 | patrickbruneel
Hi Ken, It looks like you have some solid practical experience in the transition from leaded to lead-free soldering. I hope you don�t mind me asking a question. With conventional soldering we have a library of workmanship standards available (SMT,
Electronics Forum | Tue Aug 31 07:51:28 EDT 2004 | dennispoquiz
I used to do optimization on Panasert MV2F/V,Fuji CP6/4,GSM (Universal),Sanyo TCM 3000 with no problem. My problem now is on my old Sanyo V822 SMT chipshooter. I am working on a multi-block (multi-cavity) PCB panel and i cannot, in any way, mount all
Electronics Forum | Sat Sep 18 12:10:19 EDT 2004 | Steve Gregory
I have a question about solder masking via's in a BGA pattern, and want to see if I'm thinking correctly about this. This problem is kind of along the same line as Carol's problem earlier. I think it's a bad idea to leave the via's free from solder
Electronics Forum | Fri Oct 29 04:07:27 EDT 2004 | Nick.W (TWN)
Hi, > > Has anyone had any experience with lead > free Sn-8Zn-3Bi solder paste? Apparently in Japan > it's becoming popular because it's got a melting > point of below +200C. > > Can anyone confirm that, > or does anyone have experience with >
Electronics Forum | Tue Oct 12 11:32:22 EDT 2004 | fastek
Stefen- When looking at it from your perspective only it makes no sense to off-shore. The machines and operators are but a small part that goes into the decision to move overseas. The bigger picture is the fact the "entire" operation gets outsourced.
Electronics Forum | Tue Oct 26 15:44:35 EDT 2004 | Paul_pmd
Hi Mike, Surface mount components arn't difficult to work with at all. They have pretty much the same tolorance to heat degridation as Dip packages. I suggest two Irons when working with two pole resistors and caps. Heating only one end at a time wil
Electronics Forum | Sat Nov 20 09:29:36 EST 2004 | JB
You are not giving the dimensions of the space to be used by your machines. So it's impossible to know what we are working with. But here is scenario for a very small floor space assuming that you can't have the equipment in a single line: I am ass
Electronics Forum | Thu Dec 16 12:40:48 EST 2004 | fastek
Vinit- I hate to burst your bubble regarding the FCM-1's but they will go down in history as probably the biggest platform failure in this business...based on re-sale value. For a million dollar machine to reach a level of re-sale of only $10K-$20K
Electronics Forum | Wed Jan 12 08:41:01 EST 2005 | davef
Se�or Tech QC Inspection stamps: * VRS Marking, 567 Camino Mercado Ste. A, Arroyo Grande, CA 93420, 800-782-6790 805-481-9787 Fax: 800-743-3135 Fax: 805-474-1238 contactvrs@vrsmarking.com http://www.vrsmarking.com * Des Moines Rubber Stamp Works, 8
Main Products: 1. Original new and Original Used SMT/AI Spare Parts. 2. SMT Equipments And Related Machine( SMT Calibration, SMT Feeder Carts,Conveyer etc.) 3. Maintenace and Repair Service Pre-Sales Service Provide details ab
Manufacturer's Representative / Manufacturer / Equipment Dealer / Broker / Auctions / Consultant / Service Provider
Building A, Jiepeng Square, Fuyong
Shenzhen, China
Phone: 0755-33578694