Electronics Forum | Wed Aug 10 13:31:05 EDT 2005 | patrickbruneel
Joseph, In addition to my previous post The reason why the cracks are most visible at the transformer location is due to the weight of the transformer. The stress on the boards is the highest because the weight of the transformer will warp the board
Electronics Forum | Thu Feb 16 09:00:35 EST 2006 | russ
Samir, You are a nut! I wouldn't cut your hands off! I asked because I was wondering about the stability and repeatability of the wave machine itself being used as the standard. I do understand Gage R&R or at least I think I do that was why I aske
Electronics Forum | Fri Sep 08 11:50:39 EDT 2006 | Rob
SN100C is designed not to corrode your pot, and can be used on standard solderpots (after a proper clean out), whereas SACX is still corrosive and if the coating is compromised then could cause problems. Get it in writing from the supplier that the
Electronics Forum | Fri Mar 21 08:39:38 EDT 2008 | lococost
If you are saying you're going through 1kg/h while only producing 300 pcbs a week and the rest of the time the machine is standing still, then 1.there is something seriously wrong with your machine or 2. check if an operator is suddenly covered in sh
Electronics Forum | Sun Nov 22 19:59:26 EST 2009 | prodivegsr
Hi Davef, The bubbles occurs at the body also...there's also a washing process before the conformal coating:-the Flux residue are removed after washing. ... The curing profile is also something that we are looking into during the initial troubles
Electronics Forum | Sun Nov 29 20:04:05 EST 2009 | prodivegsr
Hi sforman1, The chemical that i'm using is a solvent based coating humiseal 1B73. From my understanding,the UV curing is mainly for UV curable coating like the UV40. And the main advantage of using UV curing is for fast throughput and environment
Electronics Forum | Wed Dec 02 00:31:37 EST 2009 | jlawson
UV40 for you info was developed in Humiseal EU and has been tested heavily against Dymax product. UV40 is a great product has many approvals from major auto and whitegoods makers.... I have seen comparisons UV40 to Dymax 984LV and Dymax comes out se
Electronics Forum | Fri May 11 07:27:58 EDT 2012 | pcbprototype
Why not consider other vendors? Our China based PCB manufacturing facility is using made in China product, which is working very well. Although we are only doing PCB prototype and manufacturing, we are happy to help you source alternative from China,
Electronics Forum | Tue Dec 18 10:14:14 EST 2012 | moshesh
In those cases where we have a 3.2mm thick, 16-layer board with several GND layers, do we still need ground connection to each and every layer (with thermal relief) or, skip part of the ground patterns? Will it help soldeing rising. I can't reach mor
Electronics Forum | Wed Aug 07 16:33:08 EDT 2013 | rway
I did not see the histogram image (didn't scroll down). My point about the flat metal surfaces is they should have a large white total under top-light with red filter. You should be able to distinguish between the two (fillets and no fillets). I k