Electronics Forum | Mon Mar 10 18:21:06 EST 2003 | cman
We have both, reflow and wave solder. Planning on PTH and secondary SMT through Wave solder; then reflow primary SMT.
Electronics Forum | Thu Mar 06 17:02:40 EST 2003 | Kris
Try alpha fry technologies. http://www.frymetals.com/manufacturing/solder_reclain1.html
Electronics Forum | Mon May 17 14:14:36 EDT 2004 | cg
Or is solder quality better with automated mixing?
Electronics Forum | Thu Apr 17 16:43:09 EDT 2003 | davef
Background: * Bulwith, Ronald A., �Failure Analysis of Solder Joints�, �Insulation/Circuits� magazine, February 1978 * Banks, Donald R., et al., �The Effects of Solder Joint Voiding on Plastic Ball Grid Array Reliability�, Proceedings of the Technica
Electronics Forum | Sat Apr 19 12:00:07 EDT 2003 | modeltech
I am completely new to SMT design and for my next project I plan to use SMT for the first time. Since production volumes of the PCB's will be low, hand soldering is definitely an option, and will be necessary for my prototype PCB assembly. My proble
Electronics Forum | Mon Apr 21 08:55:35 EDT 2003 | russ
The pads you use for Reflow will be be fine for handsolder. Russ
Electronics Forum | Mon Apr 21 21:46:04 EDT 2003 | davef
We agree with Russ.
Electronics Forum | Thu May 01 16:36:49 EDT 2003 | blnorman
What is the best way to determine solder joint intermetallic composition? Metallography? XDS of the joint? Any input is appreciated.
Electronics Forum | Fri May 23 14:39:00 EDT 2003 | bradlanger
Cameron, I am burying the thermocouple in high temp solder on the solder pad of the area I want to profile.
Electronics Forum | Mon Jul 07 11:40:32 EDT 2003 | davef
If it's soldering, you have good plating.