Electronics Forum | Fri Apr 15 13:25:40 EDT 2011 | tsvetan
agree, if you have fine pitch components the placement rate will be much less of what you see in the catalogues as they quote 0805 components placemen rate. I have one year log for one of our machine which is quoted to be 6400 cps and for one year a
Electronics Forum | Tue Apr 27 09:26:43 EDT 1999 | Chrys Shea
| | | Hey MoonMan, | | | | | | Did I catch in one of your fabulous threads that you're using Tetra stencils? I'm anxious to find out how you're liking them. | | | | | | We we're all set up to go to Tetras, then mgt decided to close down our factor
Electronics Forum | Tue Apr 27 05:26:14 EDT 1999 | Charles Stringer
| | Hey MoonMan, | | | | Did I catch in one of your fabulous threads that you're using Tetra stencils? I'm anxious to find out how you're liking them. | | | | We we're all set up to go to Tetras, then mgt decided to close down our factory - Dooop!
Electronics Forum | Sun Jun 07 02:06:26 EDT 1998 | Earl Moon
| Earl, | As always, I am interested in what you have to say, but I am still a little vague on your application of ANSI Y14.5 as it relates to the manufacturability of an assembled printed circuit board. Are you implying that component placement coor
Electronics Forum | Mon Nov 27 17:47:23 EST 2000 | Dave F
Gyver: Lemme take a wack [if you�ll excuse the expression, given direction of the later discussion] at your questions. Q1. Will the baking of BGA or PCB cause more oxidation before the SMT process? A1. It certainly will not cause less oxidation,
Electronics Forum | Thu Oct 12 22:16:59 EDT 2000 | Dreamsniper
Hi Guys, I'd like to share this to all of you...you can start playing with the rests...Stated prices, if not indicated, are in Aussie $ or Singapore $. Stencil Printing Adhesive Pros a) Less Capital Equipment Cost (Short Term). In reality it is f
Electronics Forum | Thu Jun 06 09:45:14 EDT 2002 | Hussman69
We based ours on the type of paste we use (stencil life) and not so much the machine. Then we coupled that to what 'true' conditions we normally see in our plant, and determined that under these conditions Max & min) our printing process should be g
Electronics Forum | Thu Jun 06 21:35:22 EDT 2002 | ianchan
Hi mates, 1) Firstly, thanks for everyone's reply to this thread. Cheers! 2) Secondly, Hussman69: sure u dun mean that blokes' tie was too tight? musta cut off his blood flow and oxygen?!? 3) Thirdly, we checked with our paste supplier, and they r
Electronics Forum | Wed Mar 24 23:12:48 EDT 2021 | grahamcooper22
0.66 area aspect ratio...so for example...if the device is 0.5mm pitch QFP, the pcb pad may be 12 thou wide..make the aperture 9 to 10 thou wide...and reduce it's length by 10 % overall compared to the pcb pad.... Depending on device pitch, select ap
Electronics Forum | Tue Oct 09 12:23:07 EDT 2001 | Mike Konrad
Hi Danial, Yes, you can use one cleaning chemistry for all paste types. There are many available chemistries from many manufacturers. The chemistries that I would recommend include: StencilWash Plus from Aqueous Technologies http://www.aqueouste