Electronics Forum: thermal and cure and benchtop (Page 1 of 2)

Re: Reflow glue and past.

Electronics Forum | Tue Feb 08 16:09:09 EST 2000 | dean

Generally speaking with most electronic grade epoxies: 1. Cure time is a function of temperature. 2. Polymer bonds begin to quickly break down above certain temperatures (product specific). I believe aprox 170-180C. The strength of the bond de

Discoloring of Soldermask and silkscreen

Electronics Forum | Mon Apr 12 19:28:26 EDT 1999 | Tom B

Netters, When I reflow a PCB there is a discoloration of silkscreen and mask. It appears if Profile is too hot! But I dont think so, maybe I'm wrong? 1. Kester 293 no clean 2. 2.1 C/s for 30s to 150 C 3. .5 - .7 C/s for 60s to 185 C 4. 1.5 C/s u

Cracking Capacitors and Solder Balls

Electronics Forum | Mon Jun 08 14:19:30 EDT 1998 | Gary Simbulan

Earl, et al, Boy things get old and cold around here fast. I promised more detail on my capactior problem and I thought I could drop something completely different in the same message and tell a tale of solder balls. First the caps. We still have

Re: Discoloring of Soldermask and silkscreen

Electronics Forum | Wed Apr 21 00:35:31 EDT 1999 | Scott Cook

| Netters, | | When I reflow a PCB there is a discoloration of silkscreen and mask. It appears if Profile is too hot! But I dont think so, maybe I'm wrong? | | 1. Kester 293 no clean | 2. 2.1 C/s for 30s to 150 C | 3. .5 - .7 C/s for 60s to 185

Re: Discoloring of Soldermask and silkscreen

Electronics Forum | Tue Apr 13 18:11:00 EDT 1999 | Jimmy Strain

| Netters, | | When I reflow a PCB there is a discoloration of silkscreen and mask. It appears if Profile is too hot! But I dont think so, maybe I'm wrong? | | 1. Kester 293 no clean | 2. 2.1 C/s for 30s to 150 C | 3. .5 - .7 C/s for 60s to 185

Re: Discoloring of Soldermask and silkscreen

Electronics Forum | Mon Apr 19 11:21:03 EDT 1999 | Travson

| Netters, | | When I reflow a PCB there is a discoloration of silkscreen and mask. It appears if Profile is too hot! But I dont think so, maybe I'm wrong? | | 1. Kester 293 no clean | 2. 2.1 C/s for 30s to 150 C | 3. .5 - .7 C/s for 60s to 185

Re: Discoloring of Soldermask and silkscreen

Electronics Forum | Mon Apr 19 20:49:13 EDT 1999 | Dave F

| Netters, | | When I reflow a PCB there is a discoloration of silkscreen and mask. It appears if Profile is too hot! But I dont think so, maybe I'm wrong? | | 1. Kester 293 no clean | 2. 2.1 C/s for 30s to 150 C | 3. .5 - .7 C/s for 60s to 185

Re: Printing and Reflow with Ceramics

Electronics Forum | Thu Aug 13 07:53:40 EDT 1998 | Earl Moon

| | Couple of questions. | | 1) Are we talking alumina substrates as the ceramic material? | | 2) Are we co-firing gold as the conductors on the substrate surface? | | 3) In other words, is this a hybrid thick film circuit? | | 4) If so, how large or

Re: Discoloring of Soldermask and silkscreen

Electronics Forum | Tue Apr 13 18:39:24 EDT 1999 | Tom B

| | Netters, | | | | When I reflow a PCB there is a discoloration of silkscreen and mask. It appears if Profile is too hot! But I dont think so, maybe I'm wrong? | | | | 1. Kester 293 no clean | | 2. 2.1 C/s for 30s to 150 C | | 3. .5 - .7 C/s f

Re: Discoloring of Soldermask and silkscreen

Electronics Forum | Tue Apr 13 23:08:56 EDT 1999 | Jeff Sanchez

| | | Netters, | | | | | | When I reflow a PCB there is a discoloration of silkscreen and mask. It appears if Profile is too hot! But I dont think so, maybe I'm wrong? | | | | | | 1. Kester 293 no clean | | | 2. 2.1 C/s for 30s to 150 C | | | 3.

  1 2 Next

thermal and cure and benchtop searches for Companies, Equipment, Machines, Suppliers & Information

SMT feeders

High Precision Fluid Dispensers
Circuit Board, PCB Assembly & electronics manufacturing service provider

Best Reflow Oven
Voidless Reflow Soldering

High Resolution Fast Speed Industrial Cameras.
High Throughput Reflow Oven

Nozzles, Feeders, Spare Parts - Siemens, Fuji, Juki, Yamaha, etc...
Hot selling SMT spare parts and professional SMT machine solutions

Thermal Transfer Materials.