Electronics Forum | Thu Mar 04 20:14:45 EST 2010 | hallwayit
Hi, Duane, Why don't you try Tacky Flux /Tacky paste flux?
Electronics Forum | Fri Mar 12 15:13:55 EST 2010 | davesss
Thanks for the information, I will try that. Thank you
Electronics Forum | Wed Mar 24 17:09:34 EDT 2010 | davef
RE Search: Search can be tricky. Try MSD and wash
Electronics Forum | Tue May 18 02:07:39 EDT 2010 | aungthura
Hi Dave at 250'C, the leaded solder was melted.As evaluation, i just tried for sockets but not the whole boards.
Electronics Forum | Sat May 15 13:25:49 EDT 2010 | dilogic
Yeah, I tried UNIDEC, but got no response to my e-mails, so I turned to this forum...
Electronics Forum | Thu Jul 08 00:19:15 EDT 2010 | bubbobbed
thank you very much...i'll try this up...
Electronics Forum | Wed May 19 17:20:55 EDT 2010 | swag
Try stencilquik. Works good on PCB surface, not sure about component for BGA balls?
Electronics Forum | Thu Jul 08 09:48:53 EDT 2010 | jamyboy
You might try the Goodbye Chain Group. Good luck
Electronics Forum | Fri Jul 09 06:51:46 EDT 2010 | cobar
Try titanium edge stiffners on the PCB before making solder pallets.
Electronics Forum | Thu Aug 05 09:43:35 EDT 2010 | dldavis
Try antitombstone paste or if you are using nitrogen back off on the amount of nitrogen used.