Electronics Forum | Thu Jun 11 22:57:45 EDT 2009 | davef
NASA recommends baking a PCB for a minimum of 4 hours at 93+/- 5.5�C before conformally coating. [NASA-STD-8739.1, �Workmanship Standard for Staking and Conformal Coating of Printed Wiring Boards and Electronic Assemblies,� August 6, 1999]
Electronics Forum | Wed Feb 23 22:38:28 EST 2005 | davef
We: * Cure 1B73 according to spec in a heat box, like a Blue-M * Clean nozzles [one set in use, one set being cleaned] in thinner in a bronson ultrasonic cleaner * Haven't evaluated coatings in years, but would do it according to J-STD-001C, Reqmnts
Electronics Forum | Thu Jul 03 17:29:42 EDT 2008 | mikesewell
Re: item 3 - there are ultrasonic thickness machines (Panametrics makes one) that can measure coating dry with a small transducer head. A little pricey for ones that measure reliably in the .003" +/- .002" range.
Electronics Forum | Tue Jun 02 14:32:58 EDT 1998 | Chris Fontaine
We have experienced poor adhesion of acrylic conformal coating to plastic bodied IC�s. The observed symptoms of this are a blistering or lifting of the coating at the surface of the component, although peel testing has revealed that this is not alwa
Electronics Forum | Tue Jun 02 15:53:32 EDT 1998 | Earl Moon
| We have experienced poor adhesion of acrylic conformal coating to plastic bodied IC�s. The observed symptoms of this are a blistering or lifting of the coating at the surface of the component, although peel testing has revealed that this is not al
Electronics Forum | Wed Jun 03 07:13:27 EDT 1998 | Tom Tellinghuisen
| We have experienced poor adhesion of acrylic conformal coating to plastic bodied IC�s. The observed symptoms of this are a blistering or lifting of the coating at the surface of the component, although peel testing has revealed that this is not al
Electronics Forum | Tue Jun 02 17:36:43 EDT 1998 | Chris Fontaine
| | We have experienced poor adhesion of acrylic conformal coating to plastic bodied IC�s. The observed symptoms of this are a blistering or lifting of the coating at the surface of the component, although peel testing has revealed that this is not
Electronics Forum | Wed Jun 03 15:22:12 EDT 1998 | Greg Curler
| | We have experienced poor adhesion of acrylic conformal coating to plastic bodied IC�s. The observed symptoms of this are a blistering or lifting of the coating at the surface of the component, although peel testing has revealed that this is not
Electronics Forum | Tue Jun 02 18:01:47 EDT 1998 | Earl Moon
| | | We have experienced poor adhesion of acrylic conformal coating to plastic bodied IC�s. The observed symptoms of this are a blistering or lifting of the coating at the surface of the component, although peel testing has revealed that this is no
Electronics Forum | Wed Jun 17 16:54:07 EDT 2009 | jlawson
I am rep for SCS and can state.... Another system provider is SCS (Specialty Coating systems) Precision Coat Systems. Have a stable robust XYZ platform, standalone, inline configuration, Spray + Dispense and can offer Ultrasonic Nozzle Options if re