Electronics Forum: wire and bond and ceramic and pcb (Page 1 of 1)

COB and wire bond

Electronics Forum | Mon Jun 03 12:51:17 EDT 2002 | V.RAMANAND KINI

We are doing COB operations for nearly ten years. Pls. write to me if you need info on m/c selection, type of PCB, plating etc., Thanks V.RAMANAND KINI...03.06.02

COB and wire bond

Electronics Forum | Mon May 07 11:02:17 EDT 2001 | Singh

Hi all. I am looking into the implementation of the Chip on Board process with eutactic bonding and the then using either gold or aluminum wire to make wedge type wire bonding. Since I am totally new to this, can somebody guide me thru the process,

COB and Plating

Electronics Forum | Tue Oct 07 12:35:10 EDT 2008 | andy_pal

Hi All, I am using COB on my DOUBLE SIDED PCB. lastly we used Eletrolytic Ni / Flash Gold Plating. Our Boards vias Failed the UL corrosion Test. we did some cross-section analysis and found 10.75 �m of Nickel and 0.022 um of Gold and as the Process

soldering and bonding on gold PCB's

Electronics Forum | Wed Jan 09 21:19:49 EST 2002 | davef

When I said "In this area, there is no difference between your experience in ceramic substrates and PTFE substrates." I was referring to the area we were discussing ... gold plating. I am sorry if you thought I ment than the wire bonding process wa

soldering and bonding on gold PCB's

Electronics Forum | Mon Jan 07 20:37:15 EST 2002 | davef

For soldered areas, we like to keep gold thickness substantially below the maximum you propose. Search the fine SMTnet Archives for our discussions on the topic of acceptable levels of gold with solder connections. Let�s fix this �no one seems be s

soldering and bonding on gold PCB's

Electronics Forum | Wed Jan 09 12:20:00 EST 2002 | mregalia

Thanks for cluing me into IPC-2221. Though the numbers they give seem to contradict what I have learned from people working with the materials. At least I now know where the guideline for a max of 30 microinches of gold for soldering comes from. But

soldering and bonding on gold PCB's

Electronics Forum | Wed Jan 09 17:14:48 EST 2002 | mregalia

Do you bond with Al or gold wire? What happens if the Ni is over 150 microinches? Thickness of nickel is one those things that we have not been consistent with. The industry seems to pretty much universally call for 100-200 microinches. Our old board

soldering and bonding on gold PCB's

Electronics Forum | Wed Jan 09 15:24:49 EST 2002 | mregalia

Thanks Chris. As I was writing my last message our mailperson dropped off the latest issue of Circuit Assembly. It has an article on mixing SMT and COB on the same board. The author recommends as a compromise 10-20 micro inches of gold over 70-100 of

  1  

wire and bond and ceramic and pcb searches for Companies, Equipment, Machines, Suppliers & Information

Precision PCB Services, Inc
Precision PCB Services, Inc

Products, services, training, and consulting for the assembly, rework & repair of electronic assemblies. BGA process experts. Manufacturers Rep & Sole Agent in North America for Shuttle Star BGA Rework Stations.

Training Provider / Manufacturer's Representative / Equipment Dealer / Broker / Auctions / Consultant / Service Provider

1750 Mitchell Ave.
Oroville, 02

Phone: (888) 406-2830

Large PCB Dispensing System

Easily dispense fine pitch components with ±25µm positioning accuracy.
High Throughput Reflow Oven

Have you found a solution to REDUCE DISPENSE REWORK? Your answer is here.
Fluid Dispensing, Staking, TIM, Solder Paste

Software for SMT placement & AOI - Free Download.
Selective soldering solutions with Jade soldering machine

MSD Dry Cabinets


SMT & PCB Equipment - MPM, DEK, Heller, Europlacer and more...